| Molecular Dynamics Simulation of Interaction between Cuprous Oxide Crystal and Benzotriazole Derivatives |
| ;;;; |
| 山东理工大学化工学院 |
|
Cite this article:
. Molecular Dynamics Simulation of Interaction between Cuprous Oxide Crystal and Benzotriazole Derivatives. J Chin Soc Corr Pro, 2007, 27(6): 348-353 .
|
|
|
Abstract The interactions between corrosion inhibitors, i.e. benzotriazole (BTA), methyl of carboxybenzotriazole (CBTAH-ME), butyl of carboxybenzotriazole (CBTAH-BU), octyl of carboxybenzotriazole (CBTAH-OC) and Cu2O crystal have been simulated by molecular dynamics (MD). Results show that the order of binding energies of corrosion inhibitors with Cu2O crystal is as follows: CBTAH-OC>CBTAH-BU>CBTAH-ME>BTA. The analysis of various interactions and pair correlation functions of all systems indicates that binding energies are mainly determined by coulomb interaction. Benzotriazole and its derivatives are deformed during their combining with the (001) face of Cu2O crystal, and coordination bonds are formed between the copper atoms in Cu2O crystal and the nitrogen atoms in corrosion inhibitors.
|
|
Received: 22 January 2007
|
|
|
[1]Cruz J,Martinez-Aguilera L M R,Salcedo R,et al.Reactivityproperties of derivatives of 2-imidazoline:an ab initio DFT study[J].Int.J.Quantum Chem.,2001,85(4/5):546-556 [2]Bereket G,Hur E,!gretir C.Quantum chemical studies on someimidazole derivatives as corrosion inhibitors for iron in acidicmedium[J].J.Mol.Struct.(Theochem),2002,578:79-88 [3]Zhao W,Xia M Z,Lei W,et al.Quantum chemistry studies oforganophosphorus corrosion inhibitors[J].J.Chin.Soc.Corros.Prot.,2002,22(4):217-220(赵维,夏明珠,雷武等.有机膦缓蚀剂分子结构与缓蚀性能的量子化学研究[J].中国腐蚀与防护学报,2002,22(4):217-220) [4]Zhang S G,Lei W,Xia M Z,et al.QSAR study on N-containingcorrosion inhibitors:quantum chemical approach assisted by topo-logical index[J].J.Mol.Struct.(Theochem),2005,732:173-182 [5]Bartley J,Huynh N,Bottle S E,et al.Computer simulation of thecorrosion inhibition of copper in acidic solution by alkyl esters of5-carboxybenzotriazole[J].Corros.Sci.,2003,45:81-96 [6]Arshadi M R,Lashgari M,Parsafar G A.Cluster approach to cor-rosion inhibition problems:interaction studies[J].Mater.Chem.Phys.,2004,86:311-314 [7]Lashgari M,Arshadi M R.DFT studies of pyridine corrosion in-hibitors in electrical double layer:solvent,substrate,and electricfield effects[J].Chem.Phys.,2004,299:131-137 [8]Ravichandran R,Nanjundan S,Rajendran N.Effect of benzotria-zole derivatives on the corrosion of brass in Na Cl solutions[J].Appl.Surf.Sci.,2004,236:241-250 [9]Tommesani L,Brunoro G,Frignani A.On the protective action of1,2,3-benzotriazole derivative films against copper corrosion[J].Corros.Sci.,1997,39(7):1221-1237 [10]Tang S Y,Dai Y Z.Industrial Cooling Water Treatment[M].Bei-jing:Chemical Industry Press,2003(唐受印,戴友芝.工业循环冷却水处理[M].北京:化学工业出版社,2003) [11]Materials Studio 3.0.,Discover/Accelrys Software Inc.,San Diego,California,2004 [12]Sun H.COMPASS:An ab initio force field optimized for con-densed-phase application,overview with detail on alkane andbenzene compounds[J].J.Phys.Chem.B,1998,102:7338-7364 [13]Sun H,Ren P,Fried J R.The compass force field:parameteriza-tion and validation for phosphazenes[J].Comput.Theor.Polym.Sci.,1998,8(1/2):229-246 [14]Rigby D,Sun H,Eichinger B E.Computer simulations of poly(ethylene oxide):force field,pvt diagram and cyclization be-haviour[J].Polym.Int.,1998,44:311-330 [15]Burns G,Glazer A M.Space Groups for Solids State Scientists[M].Beijing:Higher Education Press,1981 [16]Mansfeld F,Smith T,Parry E P.Benzotriazole as corrosion in-hibitor for copper[J].Corrosion,1971,27:289-293 [17]Blajiev O,Hubin A.Inhibition of copper corrosion in chloridesolutions by amino-mercapto-thiadiazol and methyl-mercapto-thiadiazol:an impedance spectroscopy and a quantum-chemicalinvestigation[J].Electrochim.Acta,2004,49:2761-2770 [18]Huynh N,Bottle S E,Notoya T.Inhibition of copper corrosionby coatings of alkyl esters of carboxybenzotriazole[J].Corros.Sci.,2002,44:2583-2596 [19]Zhang S G,Lei W,Shi W Y,et al.Molecular dynamics simula-tion of interaction between calcite crystal and water-soluble poly-mers[J].Acta Phys.Chim.Sin.,2005,21(11):1193-1199(张曙光,雷武,石文艳等.水溶性聚合物与方解石晶体相互作用的MD模拟[J].物理化学学报,2005,21(11):1193-1199) [20]Heermann D W,Translated by Qin K C.Computer Simulation Meth-ods In the Theoretical Physics[M].Beijing:Peking University Press,1996(Heermann D W著,秦克成译.理论物理学中的计算机模拟方法[M].北京:北京大学出版社,1996) [21]Berendsen H J C,Postma J P M,van Gunsteren W F.Moleculardynamics with coupling to an external bath[J].J.Chem.Phys.,1984,81:3684-3690 [22]Allen M P,Tildesley D J.Computer Simulation of Liquids[M].Oxford:Clarendon Press,1987 [23]John A D.Lange's Handbook of Chemistry[M].13th ed.Knoxville:Mc Gill-Hill Press,1985 [24]Huang Y C,Hu Y J,Xiao J J,et al.Molecular dynamics simu-lation of binding energy of TATB-based PBX[J].Acta Phys.Chim.Sin.,2005,21(4):425-429(黄玉成,胡应杰,肖继军等.TATB基PBX结合能的分子动力学模拟[J].物理化学学报,2005,21(4):425-429) [25]Chen Y,Xia M Z,Lei W,et al.Quantum chemical study ofbenzotriazole and its carboxyl-alkyl esters derivatives as corrosioninhibitors[J].Mater.Prot.,2006,39(7):4-8(陈瑜,夏明珠,雷武等.苯骈三氮唑及其羧基烷基酯衍生物缓蚀性能的量子化学研究[J].材料保护,2006,39(7):4-8) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|