| Influence of Processing Temperature on Performance of Conversion Coating on AZ91D Magnesium Alloy Prepared in Phytic Acid Solution |
| DU Shiguo1, CHEN Yankun1, LU Yanling1, HUANG Xuegang1, ZHONGWeiqing2 |
1. Ordnance Engineering College of PLA, Shijiazhuang 050003;
2. No.73803 Unit of PLA, Suzhou 215156 |
|
|
|
|
Abstract AZ91D magnesium alloy, was treated in solutions of phytic acid at different temperature. SEM, Tafel and EIS were adopted and spot test was carried out to investigate the influence of processing temperature on appearance and corrosion resistance of conversion coating. Results show that the phytic acid conversion coating have better corrosion resistance when magnesium alloy was treated in a temperature range between 20 ℃ and 35 ℃. The corrosion resistance would become poor of the coatings prepared at temperature beyong the above range. The appearance of cracks on the conversion coating surface may be resulted from dehydrating in the process of desiccation. The conversion coating is a kind of coating that hinders the contact between corrosion medium and matrix metal and inhibits the diffusion of corrosion products.
|
|
Received: 16 May 2011
|
|
|
| [1] Zhao M, Wu S S, Luo J R, et al. A chromium-free conversion coating of magnesium alloy by a phosphate-permanganate solution[J]. Surf. Coat. Technol., 2006, 200(18/19): 5407[2] Tian X B, Wei C B, Yang S Q, et al. Corrosion resistance improvement of magnesium alloy using nitrogen piasmaion implantation [J]. Surf. Coat. Technol., 2005, 198(1/3): 454[3] Song G L, Jhon D S. Corrision behaviour of magnesium in ethylene glycol[J]. Corros. Sci., 2004, 46(6): 1381[4] 曾荣昌, 柯伟, 徐永波. 镁合金的最新发展及应用前景[J]. 金属学报, 2001, 37(7): 673[5] 张华, 姚广春, 刘宜汉. 镁合金无铬化学转化膜的研究进展[J]. 材料导报, 2007, 21(3): 77[6] 高瑾, 涂运骅, 李久青. 镁合金涂装保护体系失效特性及铬酸盐转化膜的影响[J]. 腐蚀科学与防护技术, 2005, 17(3): 169[7] 胡会利, 程瑾宁, 李宁等. 植酸在金属防护中的应用现状及展望[J]. 材料保护. 2005, 38(12): 39[8] 崔秀芳, 李庆芬. 镁合金表面植酸转化膜研究. I. 植酸转化膜成膜机理与耐蚀性研究[J]. 腐蚀科学与防护技术, 2007, 19(3): 203[9] Niu L Y, Jiang Z H, Li G Y, et al. A study and application of zinc phosphate coating on AZ91D magnesium alloy[J]. Surf. Coat. Technol., 2006, 200: 3021[10] Cui X F, Li Q F, Li Y, et al. Microstructure and corrosion resistance of phytic acid conversion coatings for magnesium alloy[J]. Appl. Surf. Sci., 2008, 255: 2098[11] Liu J R, Guo Y N, Huang W D. Study on the corrosion resistance of phytic acid conversion coating for magnesium alloys[J]. Surf. Coat. Technol., 2006, 201: 1536[12] Zhang S Y, Li Q, Chen B, et al. Preparation and corrosion resistance studies of nanometric sol-el-based CeO2 film with a chromium- free pretreatment on AZ91D magnesium alloy[J]. Electrochim Acta, 2009, doi: 10.1016/j. electacta.2009.07. 053[13] Luo Q L, Andrade D J. Phytic acid as all efficient low-molecular-mass displacer for anion-exchange displacement chromatography of proteins[J]. J. Chromatogr. B, 2000, 74(1): 23[14] 霍宏伟, 李瑛, 王福会. 化学转化膜上沉积镍对镁合金耐腐蚀性能的影响[J]. 中国有色金属学报, 2004, 14(2): 267[15] R F Zhang, S F Zhang, S W Duo. Influence of phytic acid concentration on coating properties obtained by MAO treatment on magnesium alloys[J]. Appl. Surf. Sci., 2009, 255: 7893 |
| No Suggested Reading articles found! |
|
|