论文

拓扑密堆μ相对含Hf的镍基粉末高温合金组织和性能的影响*

  • 张义文 ,
  • 胡本芙
展开
  • 1 钢铁研究总院高温材料研究所, 北京 100081
    2 钢铁研究总院高温合金新材料北京市重点实验室, 北京 100081
    3 北京科技大学材料科学与工程学院, 北京 100083

收稿日期: 2015-07-16

  网络出版日期: 2016-04-13

基金资助

*国家国际科技合作专项资助项目2014DFR50330

EFFECTS OF TOPOLOGICALLY CLOSE PACKED μ PHASE ON MICROSTRUCTURE AND PROPERTIES IN POWDER METALLURGY Ni-BASED SUPERALLOY WITH Hf

  • Yiwen ZHANG ,
  • Benfu HU
Expand
  • 1 High Temperature Material Institute, Central Iron and Steel Research Institute, Beijing 100081, China
    2 Beijing Key Laboratory of Advanced High Temperature Materials, Central Iron and Steel Research Institute, Beijing 100081, China
    3 School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083, China

Received date: 2015-07-16

  Online published: 2016-04-13

Supported by

Supported by International Science & Technology Cooperation Program of China (No.2014DFR50330)

摘要

研究了含Hf (0~0.89%)的FGH4097粉末高温合金中拓扑密堆μ相的析出动力学、组织形态以及μ相对Hf含量为0.30%的合金盘坯力学性能的影响. 结果表明, Hf含量为0.30%和0.89%的合金, 经750~900 ℃长期时效后μ相已明显析出. 随着时效温度的升高、时效时间的延长以及Hf添加量的增加, μ相析出量增加且尺寸长大. μ相主要在晶内以长条片状形态析出. Hf含量为0.30%的FGH4097合金盘坯在550~650 ℃长期时效后未出现μ相, 高温拉伸性能和高温持久性能没有降低, 组织稳定性良好. 750 ℃长期时效后, 盘坯中析出了μ相, 析出的μ相对高温拉伸强度无明显影响, 有助于提高高温拉伸塑性, 降低了高温持久寿命, 高温持久塑性提高约30%. 详细讨论了μ相的析出行为、γ固溶体中合金元素的再分配以及合金断口特征. 解释了μ相对力学性能影响的脆-韧双重作用机理, 并提出控制和避免μ相大量析出造成性能劣化的措施和方法.

本文引用格式

张义文 , 胡本芙 . 拓扑密堆μ相对含Hf的镍基粉末高温合金组织和性能的影响*[J]. 金属学报, 2016 , 52(4) : 445 -454 . DOI: 10.11900/0412.1961.2015.00389

Abstract

It is widely acknowledged that topologically close packed (TCP) phases are detrimental to comprehensive properties of superalloys, as TCP phases deplete strengthening elements from matrix and easily become crack initiations. In this work, the precipitation kinetics and morphology of topologically close packed μ phase in FGH4097 powder metallurgy (PM) superalloy with (0~0.89%)Hf and the effect of μ phase on the mechanical properties of FGH4097 PM superalloy billet with 0.30%Hf has been investigated. The results showed that μ phase precipitated obviously in the alloys with 0.30%Hf and 0.89%Hf after long-term ageing at 750~900 ℃, the amount and size of μ phase increased as the ageing temperature, ageing time and Hf content increasing. μ phase mainly precipitated in grains with strip and flake shapes. After long-term ageing at 550~650 ℃, no μ phase precipitated in FGH4097 PM superalloy billet with 0.30%Hf and the tensile properties and stress-rupture properties at high temperature were not decreased, which showed excellent microstructure stability. After long term ageing at 750 ℃, precipitated μ phase had little effect on tensile strength at high temperature, however, the tensile ductility increased and high temperature stress rupture life reduced, and the stress rupture ductility increased by about 20%. In this work, the precipitation behavior of μ phase, the redistribution of elements in γ solid solution and the FGH4097 PM superalloy fracture morphology characteristics have been discussed in detail. The mechanism of the brittle and ductile dual effect of μ phase on the mechanical properties has been explained. The methods of controlling and avoiding excessive μ phase precipitation which leaded to performance deterioration have been proposed.

参考文献

[1] Kotval P S, Venables J D, Calder R W.Metall Trans, 1972; 3: 457
[2] Radavich J, Furrer D, Carneiro T, Lemsky J.In: Reed R C, Green K A, Caron P, Gabb T P, Fahrmann M G, Huron E S, Woodard S A eds., Superalloys 2008, Warrendale, PA: TMS, 2008: 63
[3] Amouyal Y, Seidman D N.Acta Mater, 2011; 59: 3321
[4] Zhao S Q, Dong J X, Xie X S, Smith G D, Patel S J.In: Green K A, Pollock T M, Harada H, Howson T E, Reed R C, Schirra J J, Walston S eds., Superalloys 2004, Warrendale, PA: TMS, 2004: 63
[5] Warren R, Ingesten N G, Winberg L, R?nnhult T.Powder Metall, 1984; 27(3): 141
[6] Williams J C, Starke E A.Acta Mater, 2003; 51: 5773
[7] Ezaki H, Morinaga M, Yukawa N.Philos Mag, 1986; 53A: 709
[8] Yukawa N, Morinaga M, Ezaki H, Murata Y.In: Betz W, Brunetaud R, Coutsouradis D, Fischmeister H, Gibbons T B, Kvernes I, Lindblom Y, Marriott J B, Meadowcroft D B eds., High Temperature Alloys for Gas Turbines and Other Applications 1986, Dordrecht: D. Riedel Publishing Company, 1986: 935
[9] Morinaga M, Yukawa N, Adachi H, Ezaki H.In: Gell M, Kortovic C S, Bricknell R H, Kent W B, Radavich J F eds., Superalloys 1984, Warrendale, PA: TMS, 1984: 523
[10] Guo J T, Hou J H, Zhou L H.Metall Trans, 2006; 47: 198
[11] Qiu Y M, Zhu Y X.Acta Metall Sin, 1989; 25: 78
[11] (邱一鸣, 朱耀霄. 金属学报, 1989; 25: 78)
[12] Zhang Y W, Wang F M, Hu B F.Acta Metall Sin, 2012; 48: 187
[12] (张义文, 王福明, 胡本芙. 金属学报, 2012; 48: 187)
[13] Zhang Y W, Wang F M, Hu B F.Acta Metall Sin, 2012; 48: 1011
[13] (张义文, 王福明, 胡本芙. 金属学报, 2012; 48: 1011)
[14] Simas C T, Stoloff N S, Hagel W C. Superalloy II. New York: Joha Wiley & Sons, 1987: 143
[15] Beattie H J, Hagel W C.Trans Metall Soc AIME, 1961; 221(1): 28
[16] Miner R V.Metall Trans, 1977; 8A: 259
[17] Chen G L.Superalloy. Beijing: Metallurgical Industry Press, 1988: 70
[17] (陈国良. 高温合金. 北京:冶金工业出版社, 1988: 70)
[18] Stroh A N.Proc Royal Soc, 1954; 223A: 404
[19] Stroh A N.Proc Royal Soc London, 1955; 232A: 548
[20] Yoshinori M, Kiyoshi S, Natsuo Y.J Mater Sci, 1986; 21: 3653
[21] Boesch W J, Canada H B.J Met, 1968; 20: 46
文章导航

/

〈 〉