纳米孪晶金属塑性变形机制*

  • 卢磊 ,
  • 尤泽升
展开
  • 中国科学院金属研究所沈阳材料科学国家(联合)实验室, 沈阳110016
null

卢 磊, 女, 1970年生, 研究员, 博士

收稿日期: 2013-11-05

  修回日期: 2013-11-05

  网络出版日期: 2014-02-20

基金资助

* 国家重点基础研究发展计划项目2012CB932202以及国家自然科学基金项目51071153和51371171资助

PLASTIC DEFORMATION MECHANISMS IN NANOTWINNED METALS

  • Lei LU ,
  • Zesheng YOU
Expand
  • Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Received date: 2013-11-05

  Revised date: 2013-11-05

  Online published: 2014-02-20

Supported by

Supported by National Basic Research Program of China (No.2012CB932202) and National Natural Science Foundation of China (Nos.51071153 and 51371171)

摘要

本文综述了纳米孪晶金属材料的塑性变形机制. 通过分析纳米孪晶二维结构变形时可启动的滑移位错类型, 揭示纳米孪晶金属塑性变形的3种位错机制, 即位错塞积并穿过孪晶界机制, Shockley不全位错诱导孪晶界迁移机制以及贯穿位错在孪晶片层内受限滑移机制. 通过改变加载方向与孪晶界面的相对取向可实现这3类位错机制的可控转变.

本文引用格式

卢磊 , 尤泽升 . 纳米孪晶金属塑性变形机制*[J]. 金属学报, 2014 , 50(2) : 129 -136 . DOI: 10.3724/SP.J.1037.2013.00697

Abstract

A brief overview is provided about the plastic deformation mechanisms in nanotwinned metals. The unique two-dementional nanoscale twin lamellae lead to different dislocation slip systems activated during plastic deformation. It has been revealed that there are three distinctly different dislocation-mediated deformation mechanisms in nanotwinned metals, namely dislocation pile-up against and slip transfer across twin boundaries, Shockley partials gliding on twin boundaries leading to twin boundary migration, and threading dislocations slip confined by neighboring twin boundaries. It is further demonstrated that these three dislocation-mediated mechanisms are switchable upon changing in the loading direction with respect to twin boundaries.

参考文献

[1] Lu L, Shen Y F, Chen X H, Qian L H, Lu K. Science, 2004; 304: 422
[2] Lu K, Lu L, Suresh S. Science, 2009; 324: 349
[3] Zhu T, Li J. Prog Mater Sci, 2010; 55: 710
[4] Shen Y F, Lu L, Lu Q H, Jin Z H, Lu K.Scr Mater, 2005; 52: 989
[5] Zhang X, Misra A, Wang H, Nastasi M, Embury J D, Mitchell T E, Hoagland R G, Hirth J P. Appl Phys Lett, 2004; 84: 1096
[6] Zhang X, Misra A, Wang H, Shen T D, Nastasi M, Mitchell T E, Hirth J P, Hoagland R G, Embury J D. Acta Mater, 2004; 52: 995
[7] Lu L, Schwaiger R, Shan Z W, Dao M, Lu K, Suresh S. Acta Mater, 2005; 53: 2169
[8] Chen X H, Lu L. Scr Mater, 2007; 57: 133
[9] Chen X H, Lu L, Lu K. Scr Mater, 2011; 64: 311
[10] Lu L, You Z S, Lu K. Scr Mater, 2012; 66: 837
[11] Shute C J, Myers B D, Xie S, Barbee Jr T W, Hodge A M, Weertman J R. Scr Mater, 2009; 60: 1073
[12] Shute C J, Myers B D, Xie S, Li S Y, Barbee Jr T W, Hodge A M, Weertman J R. Acta Mater, 2011; 59: 4569
[13] Hodge A M, Furnish T A, Shute C J, Liao Y, Huang X, Hong C S, Zhu Y T, Barbee Jr T W, Weertman J R.Scr Mater, 2012; 66: 872
[14] Pan Q S, Lu Q H, Lu L. Acta Mater, 2013; 61: 1383
[15] Singh A, Tang L, Dao M, Lu L, Suresh S. Acta Mater, 2011; 59: 2437
[16] Shen Y F, Lu L, Dao M, Suresh S. Scr Mater, 2006; 55: 319
[17] Lu L, Dao M, Zhu T, Li J. Scr Mater, 2009; 60: 1062
[18] Lu L, Zhu T, Shen Y, Dao M, Lu K, Suresh S. Acta Mater, 2009; 57: 5165
[19] Wu Z X, Zhang Y W, Srolovitz D J.Acta Mater, 2009; 57: 4508
[20] Wu Z X, Zhang Y W, Srolovitz D J. Acta Mater, 2011; 59: 6890
[21] Asaro R J, Kulkarni Y. Scr Mater, 2008; 58: 389
[22] Kulkarni Y, Asaro R J. Acta Mater, 2009; 57: 4835
[23] Dao M, Lu L, Shen Y F, Suresh S.Acta Mater, 2006; 54: 5421
[24] Jerusalem A, Dao M, Suresh S, Radovitzky R. Acta Mater, 2008; 56: 4647
[25] Asaro R J, Suresh S. Acta Mater, 2005; 53: 3369
[26] Zhang X, Wang H, Chen X H, Lu L, Lu K, Hoagland R G, Misra A. Appl Phys Lett, 2006; 88: 173116
[27] Hartley C S, Blachon D L A.J Appl Phys, 1978; 49: 4788
[28] Zhu T, Gao H. Scr Mater, 2012; 66: 843
[29] Hall E O. Proc Phys Soc London, 1951; 64B: 747
[30] Petch N J.J Iron Steel Int, 1953; 174: 25
[31] Jin Z H, Gumbsch P, Ma E, Albe K, Lu K, Hahn H, Gleiter H. Scr Mater, 2006; 54: 1163
[32] Jin Z H, Gumbsch P, Albe K, Ma E, Lu K, Gleiter H, Hahn H. Acta Mater, 2008; 56: 1126
[33] Shabib I, Miller R E. Modell Simul Mater Sci Eng, 2009; 17: 055009
[34] Shabib I, Miller R E. Acta Mater, 2009; 57: 4364
[35] Lu L, Chen X, Huang X, Lu K. Science, 2009; 323: 607
[36] Li X, Wei Y, Lu L, Lu K, Gao H. Nature, 2010; 464: 877
[37] Merz M D, Dahlgren S D. J Appl Phys, 1975; 46: 3235
[38] Hodge A M, Wang Y M, Barbee Jr T W, Scr Mater, 2008; 59: 163
[39] Anderoglu O, Misra A, Wang J, Hoagland R G, Hirth J P, Zhang X. Int J Plast, 2010; 26: 875
[40] You Z S, Lu L, Lu K. Acta Mater, 2011; 59: 6927
[41] Misra A, Hirth J P, Hoagland R G. Acta Mater, 2005; 53: 4817
[42] Nix W. Metall Mater Trans, 1989; 20A: 2217
[43] Freund L B. J Appl Mech, 1987; 54: 553
[44] Matthews J W, Blakeslee A E. J Cryst Growth, 1975; 29: 273
[45] You Z, Li X, Gui L, Lu Q, Zhu T, Gao H, Lu L.Acta Mater, 2013; 61: 217
[46] Deng C, Sansoz F. Acta Mater, 2009; 57: 6090
[47] Deng C, Sansoz F. Nano Lett, 2009; 9: 1517
[48] Cao A J, Wei Y G, Mao S X. Appl Phys Lett, 2007; 90: 151909
[49] Hu Q, Li L, Ghoniem N M. Acta Mater, 2009; 57: 4866
[50] Li L, Ghoniem N M. Phys Rev, 2009; 79B: 075444
[51] Jang D, Li X, Gao H, Greer J R. Nat Nanotechnol, 2012; 7: 594
[52] Idrissi H, Wang B, Colla M S, Raskin J P, Schryvers D, Pardoen T. Adv Mater, 2011; 23: 2119
[53] Bufford D, Wang H, Zhang X.Acta Mater, 2011; 59: 93
[54] Lu K, Yan F K, Wang H T, Tao N R. Scr Mater, 2012; 66: 878
文章导航

/

〈 〉