冷坩埚定向凝固Ti44Al6Nb合金的组织演变规律 |
陈瑞润1),王纪超1,2),马腾飞1),郭景杰1),丁宏升1), 苏彦庆1),傅恒志1) |
1) 哈尔滨工业大学材料科学与工程学院, 哈尔滨150001
2) 中船重工天津修船技术研究所, 天津300456 |
|
MICROSTRUCTURE EVOLUTION OF Ti44Al6Nb ALLOY DIRECTIONALLY SOLIDIFIED WITH COLD CRUCIBLE |
CHEN Ruirun1), WANG Jichao1,2), MA Tengfei1),GUO Jingjie1), DING Hongsheng1),SU Yanqing1), FU Hengzhi1) |
1) School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001
2) Tianjin Repair Technology Research Institute, CSIC, Tianjin 300456 |
引用本文:
陈瑞润,王纪超,马腾飞,郭景杰,丁宏升, 苏彦庆,傅恒志. 冷坩埚定向凝固Ti44Al6Nb合金的组织演变规律[J]. 金属学报, 2013, 49(11): 1356-1362.
CHEN Ruirun,
WANG Jichao,
MA Tengfei,
GUO Jingjie,
DING Hongsheng,
SU Yanqing,
FU Hengzhi.
MICROSTRUCTURE EVOLUTION OF Ti44Al6Nb ALLOY DIRECTIONALLY SOLIDIFIED WITH COLD CRUCIBLE[J]. Acta Metall Sin, 2013, 49(11): 1356-1362.
[1] Lin J P, Zhao L L, Li G Y, Zhang L Q, Song X P, Ye F, Chen G L.Intermetallics, 2011; 19: 131
[2] Yang X, Xi Z P, Liu Y, Tang H, Hu K, Jia W P. Trans Nonferrerous Met Soc China, 2012; 22: 2628
[3] Song L, Zhang L Q, Xu X J, Sun J, Lin J P. Scr Mater, 2013; 68: 929
[4] Wang G, Xu L, Wang Y, Zheng Z, Cui Y Y, Yang R. Acta Metall Sin, 2011; 47: 587
(王刚, 徐磊, 王永, 郑卓, 崔玉友, 杨锐. 金属学报, 2011; 47: 587)
[5] Lin J P, Chen G L. Mater China, 2009; 28(1): 31
(林均品, 陈国良. 中国材料进展, 2009; 28(1): 31)
[6] Huang X, Qi L C, Li Z X. Rare Met Mater Eng, 2006; 35: 1845
(黄旭, 齐立春, 李臻熙. 稀有金属材料与工程, 2006; 35: 1845)
[7] Wang G, Zheng Z, Chang L T, Xu L, Cui Y Y, Yang R. Acta Metall Sin, 2011; 47: 1263
(王刚, 郑卓, 常立涛, 徐磊, 崔玉友, 杨锐. 金属学报, 2011; 47: 1263)
[8] Huang X, Qi L C, Li Z X. Rare Met Mater Eng, 2006; 35: 1848
(黄旭, 齐立春, 李臻熙. 稀有金属材料与工程, 2006; 35: 1848)
[9] Kartavykh A V, Tcherdyntsev V V, Zollinger J. Mater Chem Phys, 2010; 119: 347
[10] Zhang H R, Gao M, Tang X X, Zhang H. Acta Metall Sin, 2010; 46: 890
(张花蕊, 高明, 唐晓霞, 张虎. 金属学报, 2010; 46: 890)
[11] Luo W Z, Shen J, Min Z X, Fu H Z. Rare Met Mater Eng, 2009; 38: 1442
(罗文忠, 沈军, 闵志先, 傅恒志. 稀有金属材料与工程, 2009; 38: 1442)
[12] Yang J R, Chen R R, Ding H S, Guo J J, Su Y Q, Fu H Z. J Mater Process Technol, 2013; 213: 1355
[13] Yang J R, Chen R R, Ding H S, Guo J J, Han J C, Fu H Z.Intermetallics, 2013; 42: 184
[14] Ding H S, G J J, Chen R R, Fu H Z. Mater China, 2010; 29(2): 14
(丁宏升, 郭景杰, 陈瑞润, 傅恒志. 中国材料进展, 2010; 29(2): 14)
[15] Xiao Z X, Zheng L J, Yang L L, Yan J, Zhang H. Acta Metall Sin, 2010; 46: 1223
(肖志霞, 郑立静, 杨莉莉, 闫洁, 张虎. 金属学报, 2010; 46: 1223)
[16] Ding X F, Lin J P, Zhang L Q, Wang H L, Hao G J, Chen G L. J Alloys Compd, 2010; 506: 117
[17] Fu H Z, Guo J J, Su Y Q, Liu L, Xu D M, Li J S. Chin J Nonferrous Met, 2003; 13: 797
(傅恒志, 郭景杰, 苏彦庆, 刘林, 徐达鸣, 李金山. 中国有色金属学报, 2003; 13: 797)
[18] Saari H, Beddoes J, Seo D Y, Zhao L. Intermetallics, 2005; 13: 941
[19] Ding X F, Lin J P, Zhang L Q, Su Y Q, Chen G L. Acta Mater, 2012; 60: 498
[20] Liu D M, Li X Z, Su Y Q, Guo J J, Fu H Z. Intermetallics, 2011; 19: 175
[21] Blackburn M. Science, Techbology and Application of Titanium. London: Pergmin Press, 1970: 1
[22] Yamaguchi M, Johnson D R, Lee H N, Inui H. Intermetallics, 2000; 8: 511
[23] Murakami K, Fujiyama T, Koike A, Okamoto T. Acta Metall, 1983; 31: 1425
[24] Uhlmann D R, Seward T P, Chalmers B. Trans Metall Soc AIME, 1996; 236: 527 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|