稀土元素Gd对NiAl-Cr(Mo)-Hf共晶合金的组织和压缩性能的影响 |
梁永纯1); 郭建亭2); 盛立远2); 周兰章2) |
1) 广东电网公司电力科学研究院; 广州 510080 2) 中国科学院金属研究所; 沈阳 110016 |
|
EFFECTS OF RARE EARTH ELEMENT Gd ON THE MICROSTRUCTURE AND MECHANICAL PROPERTIES OF NiAl-Cr(Mo)-Hf EUTECTIC ALLOY |
LIANG Yongchun1); GUO Jianting2); SHENG Liyuan2); ZHOU Lanzhang2) |
1) Electric Power Research Institute of Guangdong Power Grid Corporation; Guangzhou 510080
2) Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110016 |
引用本文:
梁永纯 郭建亭 盛立远 周兰章. 稀土元素Gd对NiAl-Cr(Mo)-Hf共晶合金的组织和压缩性能的影响[J]. 金属学报, 2010, 46(5): 528-532.
,
,
.
EFFECTS OF RARE EARTH ELEMENT Gd ON THE MICROSTRUCTURE AND MECHANICAL PROPERTIES OF NiAl-Cr(Mo)-Hf EUTECTIC ALLOY[J]. Acta Metall Sin, 2010, 46(5): 528-532.
[1] Noebe R D, Bowman R R, Nathal M V. Int Mater Rev, 1993; 38: 193
[2] Johnson D R, Chen X F, Oliver B F, Noebe R D, Whittenberger J D. Intermetallics, 1995; 3: 99
[3] Darolia R. JOM, 1991; 43: 44
[4] Whittenberger J D, Locci I E, Darolia R, Bowman R R. Mater Sci Eng, 1999; A268: 165
[5] Guo J T, Cui C Y, Chen Y X, Li D X, Ye H Q. Intermetallics, 2001; 9: 287
[6] Guo J T, Huai K W, Gao Q, Ren W L, Li G S. Intermetallics, 2007; 15: 727
[7] Guo J T, Yuan C, Hou J S. Acta Metall Sin, 2008; 44: 513
(}~~, ~, (. . 2008; 44: 513)
[8] Fu H M, Wang H, Zhang H F, Hu Z Q. Scr Mater, 2006; 55: 147
[9] Li S, Zhao DQ, PanMX,WangWH. J Non–Cryst Solids, 2005; 351: 2568
[10] Xu X, Chen L Y, Zhang G Q, Wang L N, Jiang J Z. Intermetallics, 2007; 15: 1066
[11] Zheng Q, Cheng S, Strader J H, Ma E, Xu J. Scr Mater, 2007; 56: 161
[12] Xu J W. J Alloys Compd, 2008; 448: 331
[13] Wu X, Song D, Xia K. Mater Sci Eng, 2002; A329–331: 821
[14] Li W, Inkson B, Horita Z, Xia K. Intermetallics, 2000; 8: 519
[15] Xia K, Wu X, Song D. Acta Mater, 2004; 52: 841
[16] Xia K, Li W, Liu C. Scr Mater, 1999; 41: 67
[17] Walter J L, Cline H E. Metall Trans, 1970; 1: 1221
[18] George E P, Liu C T. J Mater Res, 1990; 5: 754
[19] Briant C L. Metall Trans, 1990; 21A: 2339
[20] Chen X F, Johnson D R, Noebe R D, Oliver B F. J Mater Res, 1995; 10: 1159
[21] Pop V, Coldea M, Neumann M, Chiuzbaian S, Todoran D. J Alloys Compd, 2002; 333: 1
[22] Fox A G, Tabbernor M A. Acta Metall Mater, 1991; 39: 669 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|