[an error occurred while processing this directive]
钢中第二相粒子形貌预报理论和检测方法
郭靖1,2,郭汉杰1,2(),方克明1,段生朝1,2,石骁1,2,杨文晟1,2
Morphology Prediction Theory and Experimental Measurement for the Secondary Phase Particle in Steel
Jing GUO1,2,Hanjie GUO1,2(),Keming FANG1,Shengchao DUAN1,2,Xiao SHI1,2,Wensheng YANG1,2

图6. 使用非水溶液电解后钢中非金属夹杂物的典型形貌

Fig.6. Morphologies of typical inclusion after non-aqueous solution electrolysis

(a, b) faceted Al2O3 from steel A under different magnifications (c, d) spherical or spheroidal CaO-SiO2-MnO from steel B under different magnifications