Morphology Prediction Theory and Experimental Measurement for the Secondary Phase Particle in Steel
|
|
图5. A钢中Al2O3、MgAl2O4和TiN典型形貌 |
Fig.5. Typical morphologies of Al2O3 with α=3.06~6.12 (a, b), MgAl2O4 with α=4.06~8.12 (c, d) and TiN with α=3.15~6.29 (e, f) inclusions in steel A (a) polyhedral (b) spheroidal (c) polyhedral (d) spheroidal (e) cubic (f) gear-like |
![]() |