钢中第二相粒子形貌预报理论和检测方法
|
|
Morphology Prediction Theory and Experimental Measurement for the Secondary Phase Particle in Steel
|
|
图1. 不同Jackson α指数时晶体/熔体界面相对自由能与界面晶体原子占比的关系 |
Fig.1. Relations between crystal/melt interface relative energy and fraction of crystal lattice atom (X) with different Jackson α factors (ΔF—crystal/melt interface free energy, N—the number of crystal lattice on the crystal/melt interface, k—Boltzman constant, T—temperature) |
![]() |