Al-Si-Ge钎料钎焊Cu/Al接头组织与性能研究
牛志伟,叶政,刘凯凯,黄继华(
),陈树海,赵兴科
Microstructure and Property of Cu/Al Joint Brazed with Al-Si-Ge Filler Metal
Zhiwei NIU,Zheng YE,Kaikai LIU,Jihua HUANG(
),Shuhai CHEN,Xingke ZHAO
图6. 典型的Cu/Al钎焊接头断裂位置的SEM像
Fig.6. Typical SEM image of the fracture position of the Cu/Al joint