图5. Al-5.6Si-25.2Ge和Zn-22Al钎料钎焊Cu/Al接头断口的SEM像
Fig.5. SEM images of the fracture surface of the Cu/Al joints brazed with Al-5.6Si-25.2Ge (a) and Zn-22Al (b) filler metals