热处理对连续点式锻压激光快速成形GH4169合金组织与拉伸性能的影响
席明哲(),周玮,尚俊英,吕超,吴贞号,高士友
Effect of Heat Treatment on Microstructure and Mechanical Properties of Consecutive Point-Mode Forging and Laser Rapid Forming GH4169 Alloy
Mingzhe XI(),Wei ZHOU,Junying SHANG,Chao LV,Zhenhao WU,Shiyou GAO

图5. 经980STA、1020STA、1050STA 和1080STA热处理后,GH4169合金试样的显微硬度

Fig.5. Microhardness of CPF-LRF GH4169 alloy after 980STA, 1020STA, 1050STA and 1080STA heat treatments