Fig.2. Microstructures and EDS analyses of CPF-LRF GH4169 alloy heat treated by 980STA (a) columnar crystals (b) Laves phase and δ phase (c) EDS analysis of Laves phase pointed by arrow 1 in Fig.2b (d) EDS analysis of δ phase pointed by arrow 2 in Fig.2b