国产核电安全端异种金属焊接件的微观结构及局部性能研究
|
明洪亮 1,2,张志明 1,王俭秋 1( ),韩恩厚 1,苏明星 3
|
Microstructure and Local Properties of a Domestic Safe-End Dissimilar Metal Weld Joint by Using Hot-Wire GTAW
|
Hongliang MING 1,2,Zhiming ZHANG 1,Jianqiu WANG 1( ),En-Hou HAN 1,Mingxing SU 3
|
|
图3. 慢应变速率拉伸实验试样尺寸示意图
|
Fig.3. Schematic of U-notched round-bar sample used for slow strain rate test (unit: mm) |
|
|
|
|