国产核电安全端异种金属焊接件的微观结构及局部性能研究
|
明洪亮 1,2,张志明 1,王俭秋 1( ),韩恩厚 1,苏明星 3
|
Microstructure and Local Properties of a Domestic Safe-End Dissimilar Metal Weld Joint by Using Hot-Wire GTAW
|
Hongliang MING 1,2,Zhiming ZHANG 1,Jianqiu WANG 1( ),En-Hou HAN 1,Mingxing SU 3
|
|
图19. 焊接件不同部位在模拟核电高温高压水环境中慢应变速率拉伸实验结果
|
Fig.19. Stress-extension curves of local areas in the DMWJ obtained by slow strain rate test (SSRT) conducted in simulated primary water containing 1500 mg/L B as H3BO3 and 2.3 mg/L Li as LiOH with 2 mg/L dissolved oxygen at 325 ℃ |
|
|
|
|