国产核电安全端异种金属焊接件的微观结构及局部性能研究
|
明洪亮 1,2,张志明 1,王俭秋 1( ),韩恩厚 1,苏明星 3
|
Microstructure and Local Properties of a Domestic Safe-End Dissimilar Metal Weld Joint by Using Hot-Wire GTAW
|
Hongliang MING 1,2,Zhiming ZHANG 1,Jianqiu WANG 1( ),En-Hou HAN 1,Mingxing SU 3
|
|
图14. 沿图1b中L1线的显微硬度分布及界面处显微硬度压痕
|
Fig.14. Microhardness distribution along the DMWJ across L1 (as labeled in Fig.1b) (a) and the indentations in the interface (b, c) |
|
|
|
|