Fig.5. The projection of an inclined {101?2} twin boundary [69] (w—width of projection, t—thickness of sample) (a) dark field TEM image showing a band-like twin boundary (b) schematic illustrates that the band-like feature comes from the projection of a inclined twin boundary along the e-beam direction |