先进金属材料的第二相强化*
|
吕昭平( ),蒋虽合,何骏阳,周捷,宋温丽,吴渊,王辉,刘雄军
|
SECOND PHASE STRENGTHENING IN ADVANCED METAL MATERIALS
|
Zhaoping LU( ),Suihe JIANG,Junyang HE,Jie ZHOU,Wenli SONG,Yuan WU,Hui WANG,Xiongjun LIU
|
|
图16. (Cu0.5Zr0.5)100-xAlx (x=0, 4, 6, 原子分数, %)非晶合金的DSC升温降温曲线及其过冷奥氏体等温转变曲线(TTT)图[18]
|
Fig.16. DSC heating and cooling curves (a) and schematic time-temperature-transformation (TTT) diagram (b) of (Cu0.5Zr0.5)100-xAlx (x=0, 4, 6, atomic fraction, %) alloy[18] (Ms—martensitic transformation start temperature, As—autensite transformation start temperature, Tg—glass transition temperature, TL—liquidus temperature) |
|
|
|
|