热变形和淬火配分处理的复合作用对低碳合金钢马氏体相变机制的影响*
|
THE COMBINED EFFECT OF HOT DEFORMATION PLUS QUENCHING AND PARTITIONING TREATMENT ON MARTENSITE TRANSFORMATION OF LOW CARBON ALLOYED STEEL
|
(a) combined process (b) conventional two-step Q&P process |