| ALPHA-PHASE MICROCRYSTALLINE STRUCTURE OF IONITRIDING LAYER ON STEELS |
| LI Ji;YUAN Yongsheng Northeast University of Technology; Shenyang; YUAN Keqi University of Science and Technology Beijing |
|
Cite this article:
LI Ji;YUAN Yongsheng Northeast University of Technology; Shenyang; YUAN Keqi University of Science and Technology Beijing. ALPHA-PHASE MICROCRYSTALLINE STRUCTURE OF IONITRIDING LAYER ON STEELS. Acta Metall Sin, 1991, 27(5): 148-150.
|
|
|
Abstract TEM observation on the ionitriding layer was carried out of 3 different steels W18Cr4V, 38CrMoAl and 1Cr18Ni9Ti. And AES of elementary analysis was also made of the outer surface of ionitiding layer on austenite stainless steel. Perhaps due to the ion-bombardment effect, a microcrystalline strucure with texture was affirmed along surface of the ionitriding layer. It may be affected by cathodic sputtering and adsorption that the atomic ratio of Cr/ Fe increases and of Ni/Fe decrease on surface of nitriding layer on austenitic stainless steel 1Cr18Ni9Ti, thus the α-phase microcrystalline structure is also occurred.
|
|
Received: 18 May 1991
|
1 Larsen B. Fφrland T. Mol Phys. 1973: 26: 1521 2 陈念贻,徐驰,李通化,江乃雄.中国科学(B辑),1987;(1) :21 3 徐驰,江乃雄,陈念贻.化学学报,1989:47:529 4 徐驰,陈念贻,江乃雄.物理化学学报,1987;3:55 5 Sangster M J L, Dixon M. Adv Phys, 1976; 25: 247 6 Holm J L, Kleppa O J. J Chem Phys, 1968; 49: 2425 7 Lumsden J. In: Inman D, Lovering D G eds., Ionic Liquids, New York: Plenum, 1981: 27--56 8 Fφrland T. J Phys Chem, 1955; 59: 152 9 Blander M. Molten Salt Chemistry, New York: Interscience, 1964: 127 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|