摘要: 研究了磁控溅射NiAl微晶涂层对NiAl-TiC(20%, 体积分数)复合材料1000-1100℃高温氧化性能的影响. 结果表明, NiAl微晶涂层大大提高了NiAl-TiC复合材料的恒温及循环氧化性能, 降低氧化速率几个数量级, 对于NiAl-TiC复合材料来说, 其表面形成以TiO2为主的复合氧化物, 而施加NiAl微晶涂层后, 其表面氧化物主要是Al2O3.
关键词 NiAl微晶涂层NiAl-TiC复合材料    
Key words
收稿日期: 2000-03-10     
ZTFLH:  TG174.445 TG172.82  
[1] Miracle D B. Acta Metall Mater,1993; 41: 649
[2] Vedula K, Pathave V, Aslanidis I, TiTran R H. Mat ResSoc Symp Proc,1986; 39: 411
[3] Vedula K, Stephens J R. Mat Res Soc Symp Proc, 1987;81: 381
[4] Kumar K S, Whittenberger J D. Moter Sci Technol,1992;8: 317
[8] Whittenberger J D, Viswanadham R K, Mannan S K,Sprissler B. J Mater Sci, 1990; 25: 35
[6] Wang L, Aresenault R J. Mater Sci Egg, 1990; A127: 91
[7] Whittenberger J D, Kumar K S, Mannan S K. Mater HighTemp,1991; 9: 3
[8] Alman D E, Stoloff N S. Int J Powder Metall , 1991; 27:29
[9] Xing Z P, Dai J Y, Guo J T, An G Y, Hu Z Q. ScriptaMetall Mater, 1994; 31: 1141
[10] Xing Z P, Yu L G, Guo J T, J,Dai Y, An G Y, Ha ZQ. J Mater Sci Lett, 1995; 14: 443
[11] Baker i, Munroe P R. J Met, 1988; 40: 28
[12] Xing Z P, Guo J T, Han Y F, Yu L G. Metall Moter Trans,1997; 28A: 1079
[13] Guo J T, Xing Z P, Wang S H, Li H. J Iron Steel Res,1997; 9: 23(郭建亭.邢占平,王淑荷,李辉.钢铁研究学报增刊.1997;9:23)
[14] Xing Z P, Guo J T, Hu Z Q, An G Y. Acta Metall Sin,1994; 7: 45
[15] Xing Z P, Yu L G, Guo J T, Dai J Y, An G Y, Hu Z Q.'J Mater Sci Lett, 1996; 14: 443
[16] Jiang D T. Doctoral Thesis, Institute of Metal Research,The Chinese Academy of Sciences, Shenyang,1998: 12(姜东涛.博士学位论文,中国科学院金属研究所,沈阳,1998:12)
[17] TIng Z L, Wang F H, Wu W T. Oxid Met, 1997; 48: 511
[18] Yang S L, Wang F H. Acta Metall Sin, 2000; 36: 511(杨松岚,王福会.金属学报,2000;36:511)
[19] Gesmundo F, Viani F, Niu Y, Douglass D L. Oxid Met,1994; 39:197
[20] Gesmundo F, Viani F, Niu Y. Oxid Met,1994; 42: 285
[21] Gesmundo F, Viani F, Niu Y, Douglas. D L. Oxid Met,1994; 42: 409
[22] Gesmundo F, Viani F, Niu Y. Oxid Met, 1994; 42: 465
[23] Niu Y, Gesmundo F, Viani F, Wu W T. Oxid Met, 1997;47: 21
[24] Rahmal A, Spencer P J. Oxid Met, 1991; 35: 53
[25] Backer S, Rahmel A, Schorr M, Schutze M. Oxid Met,1992; 38: 425
[1] 徐春梅; 郭建亭 . NiAl微晶涂层对两种NiAl基共晶合金高温氧化性能的影响[J]. 金属学报, 2002, 38(7): 673-678 .
[2] 杨松岚; 王福会; 朱圣龙 . 柱状晶界面对溅射NiAl微晶涂层高温氧化性能的影响[J]. 金属学报, 2001, 37(6): 625-627 .