定向凝固镍基高温合金DZ466表面CoAl涂层的氧化及组织演变 |
任维鹏1(), 李青1, 黄强1, 肖程波1, 何利民2 |
1 北京航空材料研究院先进高温结构材料重点实验室 北京 100095 2 北京航空材料研究院航空材料先进腐蚀与防护航空科技重点实验室 北京 100095 |
|
Oxidation and Microstructure Evolution of CoAl Coating on Directionally Solidified Ni-Based Superalloys DZ466 |
Weipeng REN1(), Qing LI1, Qiang HUANG1, Chengbo XIAO1, Limin HE2 |
1 Science and Technology on Advanced High Temperature Structural Materials Laboratory, Beijing Institute of Aeronautical Materials, Beijing 100095, China 2 Aviation Key Laboratory of Science and Technology on Advanced Corrosion and Protection for Aviation Materials, Beijing Institute of Aeronautical Materials, Beijing 100095, China |
引用本文:
任维鹏, 李青, 黄强, 肖程波, 何利民. 定向凝固镍基高温合金DZ466表面CoAl涂层的氧化及组织演变[J]. 金属学报, 2018, 54(4): 566-574.
Weipeng REN,
Qing LI,
Qiang HUANG,
Chengbo XIAO,
Limin HE.
Oxidation and Microstructure Evolution of CoAl Coating on Directionally Solidified Ni-Based Superalloys DZ466[J]. Acta Metall Sin, 2018, 54(4): 566-574.
[1] | Liu L, Yang F, Wu Y.Preparation of Si-modified aluminide coating by CVD process[J]. Heat Treat. Met., 2016, 41(7): 79(刘磊, 杨甫, 吴勇. 硅改性铝化物涂层的CVD制备工艺[J]. 金属热处理, 2016, 41(7): 79) | [2] | Dai J W, Yi J, Wang Z K, et al.High temperature oxidation behavior of Pt modified aluminide coating on single crystal superalloy[J]. J. Aeronaut. Mater., 2015, 35(5): 32(戴建伟, 易军, 王占考等. 单晶高温合金铂改性铝化物涂层的高温氧化行为[J]. 航空材料学报, 2015, 35(5): 32) | [3] | Song P, Lu J S, Lv J G, et al.Influence factors of high temperature oxidation for Pt-modified-aluminide bond coatings[J]. Rare Met. Mater. Eng., 2010, 39: 304(宋鹏, 陆建生, 吕建国等. 铂铝涂层高温氧化的影响因素研究[J]. 稀有金属材料与工程, 2010, 39: 304) | [4] | Xu Z H, Dai J W, Niu J, et al.Influence of deposition temperature on the phase structure and morphology of aluminide coatings[J]. Corros. Prot., 2013, 34: 991(许振华, 戴建伟, 牛静等. 沉积温度对铝化物涂层相结构与微观形貌的影响[J]. 腐蚀与防护, 2013, 34: 991) | [5] | Mahesh R A, Jayaganthan R, Prakash S, et al.High temperature cyclic oxidation behavior of magnetron sputtered Ni-Al thin films on Ni- and Fe-based superalloys[J]. Mater. Chem. Phys., 2009, 114: 629 | [6] | Li H X, Qiao M, Zhou C G.Formation and cyclic oxidation resistance of Hf-Co-modified aluminide coatings on nickel base super-alloys[J]. Mater. Chem. Phys., 2014, 143: 915 | [7] | Liu Z J, Zhao X S, Guo H M, et al.Cyclic oxidation resistance of Ce/Co modified aluminide coatings on nickel base superalloys[J]. Corros. Sci., 2015, 94: 135 | [8] | Qiao M, Zhou C G.Hot corrosion behavior of Co modified NiAl coating on nickel base superalloys[J]. Corros. Sci., 2012, 63: 239 | [9] | Pei Y W, Zhou C G.Improved hot corrosion resistance of Dy-Co-modified aluminide coating by pack cementation process on nickel base superalloy[J]. Corros. Sci., 2016, 112: 710 | [10] | Liu Z J, Zhao X S, Zhou C G.Improved hot corrosion resistance of Y-Ce-Co-modified aluminide coating on nickel base superalloys by pack cementation process[J]. Corros. Sci., 2015, 92: 148 | [11] | Wu D L, Zhang H Y, Wei H, et al.Hot corrosion behavior of four modified aluminide coatings on DZ38G alloy[J]. J. Chin. Soc. Corros. Prot., 2014, 34: 502(吴多利, 张洪宇, 韦华等. 4种改性的铝化物涂层对DZ38G合金热腐蚀性能的影响[J]. 中国腐蚀与防护学报, 2014, 34: 502) | [12] | Chen J H, Little J A.Degradation of the platinum aluminide coating on CMSX4 at 1100 ℃[J]. Surf. Coat. Technol., 1997, 92: 69 | [13] | Pint B A, Zhang Y.Performance of Al-rich oxidation resistant coatings for Fe-base alloys[J]. Mater. Corros., 2015, 62: 549 | [14] | Shen M L, Zhu S L.Advancement of technologies for preparing high-performance aluminide coatings[J]. Aeronaut. Manuf. Technol., 2016, 21: 105(沈明礼, 朱圣龙. 先进铝化物涂层制备技术进展[J]. 航空制造技术, 2016, 21: 105) | [15] | Li W Y, Jiang R R, Huang C J, et al.Effect of cold sprayed Al coating on mechanical property and corrosion behavior of friction stir welded AA2024-T351 joint[J]. Mater. Des., 2015, 65: 757 | [16] | Mohammadi I, Afshar A.Modification of nanostructured anodized aluminum coatings by pulse current mode[J]. Surf. Coat. Technol., 2015, 278: 48 | [17] | Huang L, Sun X F, Guan H R, et al.Degradation behavior of aluminide coating on directionally solidified nickel base superalloy M951[J]. Corros. Sci. Prot. Technol., 2005, 17: 34(黄粮, 孙晓峰, 管恒荣等. 定向凝固高温合金M951低压渗铝涂层的高温氧化及相变过程[J]. 腐蚀科学与防护技术, 2005, 17: 34) | [18] | Ren W P, Xiao C B, Li Q, et al.Microstructure evolution of cobalt aluminide coating on nickel-based superalloys during exposure at 1050 ℃[J]. Vacuum, 2014, 106: 39 | [19] | Ren W P, Li Q, Song J X, et al. Oxidation and microstructure evolution of cobalt aluminide coatings on directionally solidified superalloys during long term exposure at 1000 ℃[J]. Mater. Res. Innovat., 2014, 18(S4): S4-945-S4-951 | [20] | Rabiei A, Evans A G.Failure mechanisms associated with the thermally grown oxide in plasma sprayed thermal barrier coatings[J]. Acta Mater., 2000, 48: 3963 | [21] | Puetz P, Huang X A, Lima R S, et al.Characterization of transient oxide formation on CoNiCrAlY after heat treatment in vacuum and air[J]. Surf. Coat. Technol., 2010, 205: 647 | [22] | Felten E J, Pettit F S.Development, growth, and adhesion of Al2O3 on platinum-aluminum alloys[J]. Oxid. Met., 1976, 10: 189 | [23] | Wada K, Yamaguchi N, Matsubara H.Effect of substrate rotation on texture evolution in ZrO2-4 mol. % Y2O3 layers fabricated by EB-PVD[J]. Surf. Coat. Technol., 2005, 191: 367 | [24] | Bourban S, Karapatis N, Hofmann H, et al.Solidification microstructure of laser remelted Al2O3-ZrO2 eutectic[J]. Acta Mater., 1997, 45: 5069 | [25] | Angenete J, Stiller K.Oxidation of simple and Pt-modified aluminide diffusion coatings on Ni-base superalloys—II. Oxide scale failure[J]. Oxid. Met., 2003, 60: 83 | [26] | Liu G M, Li M S, Ma J H, et al.Transient oxidation behavior of nanocrystalline CoCrAlY coating at 1050 ℃[J]. Trans. Nonferrous Met. Soc. China, 2007, 17: 595 | [27] | Grabke H J, Bramm M W, Wagemann B.The oxidation of NiAl[J]. Mater. Corros., 1996, 47: 675 | [28] | Brumm M W, Grabke H J.The oxidation behaviour of NiAl—I. Phase transformations in the alumina scale during oxidation of NiAl and NiAl-Cr alloys[J]. Corros. Sci., 1992, 33: 1677 | [29] | Pint B A, Martin J R, Hobbs L W.The oxidation mechanism of θ-Al2O3 scales[J]. Solid State Ionics, 1995, 78: 99 | [30] | Balmain J, Loudjani M K, Huntz A M.Microstructural and diffusional aspects of the growth of Alumina scales on β-NiAl[J]. Mater. Sci. Eng., 1997, A224: 87 | [31] | Manap A, Nakano A, Ogawa K.The protectiveness of thermally grown oxides on cold sprayed CoNiCrAlY bond coat in thermal barrier coating[J]. J. Therm. Spray Technol., 2012, 21: 586 | [32] | Guo H B, Cui Y J, Peng H, et al.Improved cyclic oxidation resistance of electron beam physical vapor deposited nano-oxide dispersed beta-NiAl coatings for Hf-containing superalloy[J]. Corros. Sci., 2010, 52: 1440 | [33] | Zhang L C, Heuer A H.Microstructural evolution of the nickel platinum-aluminide bond coat on electron-beam physical-vapor deposition thermal-barrier coatings during high-temperature service[J]. Metall. Mater. Trans., 2005, 36A: 43 | [34] | Gale W F, King J E. Microstructural development in aluminide diffusion coatings on nickel-base superalloy single crystals [J]. Surf. Coat. Technol., 1992, 54-55: 8 | [35] | Basuki E, Crosky A, Gleeson B.Interdiffusion behaviour in aluminide-coated René 80H at 1150 ℃[J]. Mater. Sci. Eng., 1997, A224: 27 | [36] | Holmes J W, McClintock F A. The chemical and mechanical processes of thermal fatigue degradation of an aluminide coating[J]. Metall. Trans., 1990, 21A: 1209 | [37] | Zhang Y H, Knowles D M, Withers P J.Microstructural development in Pt-aluminide coating on CMSX-4 superalloy during TMF[J]. Surf. Coat. Technol., 1998, 107: 76 | [38] | González M A, Martínez D I, Saucedo C T, et al.Microstructural evolution of Pt-aluminide coating influencedby cycle oxidation service conditions[J]. Eng. Fail. Anal., 2013, 29: 122 | [39] | Ross E W, Sims C T. Superalloys II, Nickel-Base Alloys[M]. New York: Wiley, 1987: 98 | [40] | Guo J T.Materials Science and Engineering for Superalloys [M]. Beijing: Science Press, 2008: 92(郭建亭. 高温合金材料学 [M]. 上册. 北京: 科学出版社, 2008: 92) | [41] | Kong Y H, Chen Q Z.Effect of minor additions on the formation of TCP phases in modified RR2086 SX superalloys[J]. Mater. Sci. Eng., 2004, A366: 135 |
|
|