非等温回归再时效对Al-8Zn-2Mg-2Cu合金厚板组织及性能的影响 |
冯迪1(), 张新明2, 陈洪美1, 金云学1, 王国迎1 |
1 江苏科技大学材料科学与工程学院 镇江 212003 2 中南大学材料科学与工程学院 长沙 410083 |
|
Effect of Non-Isothermal Retrogression and Re-Ageing on Microstructure and Properties of Al-8Zn-2Mg-2Cu Alloy Thick Plate |
Di FENG1(), Xinming ZHANG2, Hongmei CHEN1, Yunxue JIN1, Guoying WANG1 |
1 School of Materials Science and Engineering, Jiangsu University of Science and Technology, Zhenjiang 212003, China 2 School of Materials Science and Engineering, Central South University, Changsha 410083, China |
引用本文:
冯迪, 张新明, 陈洪美, 金云学, 王国迎. 非等温回归再时效对Al-8Zn-2Mg-2Cu合金厚板组织及性能的影响[J]. 金属学报, 2018, 54(1): 100-108.
Di FENG,
Xinming ZHANG,
Hongmei CHEN,
Yunxue JIN,
Guoying WANG.
Effect of Non-Isothermal Retrogression and Re-Ageing on Microstructure and Properties of Al-8Zn-2Mg-2Cu Alloy Thick Plate[J]. Acta Metall Sin, 2018, 54(1): 100-108.
[1] | Paul A R, Zhang Y, Knight S.Heat treatment of 7xxx series aluminium alloys—Some recent developments[J]. Trans. Nonferrous Met. Soc. China, 2014, 24: 2003 | [2] | Zhang X M, Deng Y L, Zhang Y.Development of high strength aluminum alloys and processing techniques for the materials[J]. Acta Metall. Sin., 2015, 51: 257(张新明, 邓运来, 张勇. 高强铝合金的发展及其材料的制备加工技术[J]. 金属学报, 2015, 51: 257) | [3] | Grong ?, Shercliff H R.Microstructural modelling in metals processing[J]. Prog. Mater. Sci., 2002, 47: 163 | [4] | Hutchinson C R, Gouné M, Redja?mia. A Selecting non-isothermal heat treatment schedules for precipitation hardening systems: An example of coupled process-property optimization[J]. Acta Mater., 2007, 55: 213 | [5] | Jiang D M, Liu Y, Liang S, et al.The effects of non-isothermal aging on the strength and corrosion behavior of AlZnMgCu alloy[J]. J. Alloys Compd., 2016, 681: 57 | [6] | Marlaud T, Deschamps A, Bley F, et al.Evolution of precipitate microstructures during the retrogression and re-ageing heat treatment of an Al-Zn-Mg-Cu alloy[J]. Acta Mater., 2010, 58: 4814 | [7] | Staley J T.Method and process of non-isothermal aging for aluminum alloys [P]. Durham US Pat, 0237113Al, 2007 | [8] | Li K, Zhang K, Yang L, et al.Investigation of non-isothermal aging process of 7085 aluminum alloy [A]. Proceedings of the 12th International Conference on Aluminium Alloys[C]. Yokohama: The Japan Institute of Light Metals, 2010: 2120 | [9] | Zhen L, Huang M, Liu M, et al.Effect of cooling method on the microstructure and properties of 7085 aluminum alloy during non-isothermal aging [A]. Proceedings of the 12th International Conference on Aluminium Alloys[C]. Yokohama: The Japan Institute of Light Metals, 2010: 481 | [10] | Jiang J T, Xiao W Q, Yang L, et al.Ageing behavior and stress corrosion cracking resistance of a non-isothermally aged Al-Zn-Mg-Cu alloy[J]. Mater. Sci. Eng., 2014, A605: 167 | [11] | Liu Y, Jiang D M, Li B Q, et al.Effect of cooling aging on microstructure and mechanical properties of an Al-Zn-Mg-Cu alloy[J]. Mater. Des., 2014, 57: 79 | [12] | Liu Y, Jiang D M, Li B Q, et al.Heating aging behavior of Al-8.35Zn-2.5Mg-2.25Cu alloy[J]. Mater. Des., 2014, 60: 116 | [13] | Peng X Y, Guo Q, Liang X P, et al.Mechanical properties, corrosion behavior and microstructures of a non-isothermal ageing treated Al-Zn-Mg-Cu alloy[J]. Mater. Sci. Eng., 2017, A688: 146 | [14] | Koziel J, Blaz L, Wloch G, et al.Precipitation processes during non-isothermal aging of fine-grained AA2219[J]. J. Alloys Compd., 2016, 682: 468 | [15] | Cina B.Reducing the susceptibility of alloys, particularly aluminium alloys, to stress corrosion cracking [P].US Pat, 3856584, 1974 | [16] | Feng D, Zhang X M, Liu S D, et al.The effect of pre-ageing temperature and retrogression heating rate on the microstructure and properties of AA7055[J]. Mater. Sci. Eng., 2013, A588: 34 | [17] | Su R M, Qu Y D, Li D R.Pre-aging of retrogression and re-aging of spray formed 7075 alloy[J]. Acta Metall. Sin., 2014, 50: 863(苏睿明, 曲迎东, 李荣德. 喷射态7075合金回归再时效中预时效的研究[J]. 金属学报, 2014, 50: 863) | [18] | Starink M J, Li X M.A model for the electrical conductivity of peak-aged and overaged Al-Zn-Mg-Cu alloys[J]. Metall. Mater. Trans., 2003, 34A: 899 | [19] | Chen J Z.Ageing precipitation behavior and mechanical properties of AA7055 aluminum alloy [D]. Harbin: Harbin Institute of Technology, 2008(陈军洲. AA7055 铝合金的时效析出行为与力学性能 [D]. 哈尔滨: 哈尔滨工业大学, 2008) | [20] | Feng D, Zhang X M, Liu S D, et al.Effect of pre-aging temperature and retrogression heating rate on microstructure and properties of 7150 alloy[J]. Chin. J. Nonferrous Met., 2013, 23: 1173(冯迪, 张新明, 刘胜胆等. 预时效温度及回归加热速率对7150铝合金显微组织及性能的影响[J]. 中国有色金属学报, 2013, 23: 1173) | [21] | Ning A L, Liu Z Y, Feng C, et al.Analysis on the behavior of exceeding peak aging strength of aluminum alloy at condition of retrogression and reaging[J]. Acta Metall. Sin., 2006, 42: 1253(宁爱林, 刘志义, 冯春等. 铝合金回归再时效状态的超峰时效强度行为分析[J]. 金属学报, 2006, 42: 1253) | [22] | Feng D, Zhang X M, Liu S D, et al.Non-isothermal retrogression kinetics for grain boundary precipitate of 7A55 aluminum alloy[J]. Trans. Nonferrous Met. Soc. China, 2014, 24: 2212 | [23] | Feng D, Zhang X M, Liu S D, et al.Non-isothermal “retrogression and re-ageing” treatment schedule for AA7055 thick plate[J]. Mater. Des., 2014, 60: 208 | [24] | Cui Z Q, Qin Y C.Metallography & Heat Treatment [M]. Beijing: Mechanical Industry Press, 2012: 179(崔忠圻, 覃耀春. 金属学与热处理 [M]. 北京: 机械工业出版社, 2012: 179) | [25] | Lumley R.Fundamentals of Aluminium Metallurgy [M]. London: Woodhead Publishing Ltd., 2011: 356 | [26] | Cui X L, Wu Y Y, Zhang G J, et al.Study on the improvement of electrical conductivity and mechanical properties of low alloying electrical aluminum alloys[J]. Composites, 2017, 110B: 381 | [27] | Zhang G Y, Zhang H, Fang G L, et al.Electronic structure of different regions and analysis of stress corrosion mechanism of Al-Zn-Mg-Cu alloys[J]. Acta Metall. Sin., 2009, 45: 687(张国英, 张辉, 方戈亮等. Al-Zn-Mg-Cu系铝合金中不同区域电子结构及应力腐蚀机理分析[J]. 金属学报, 2009, 45: 687) |
|
|