准晶磨料的“碾抹”特性对软金属表面的平整性、硬度及耐蚀性的影响* |
陈永君1,胡小刚1,羌建兵1,2,董闯1,2() |
1 大连理工大学材料科学与工程学院, 大连 116024
2 大连理工大学三束材料改性教育部重点实验室, 大连 116024 |
|
QUASICRYSTAL ABRASIVE POLISHING ON SOFT METALS VIA A CHARACTERISTIC SMEARING WEAR MECHANISM FOR EFFICIENT SURFACE FLATTENING, HARDENING AND CORROSION ENHANCEMENT |
Yongjun CHEN1,Xiaogang HU1,Jianbing QIANG1,2,Chuang DONG1,2() |
1 School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024, China
2 Key Lab of Materials Modification by Laser, Ion and Electron Beams, Ministry of Education, Dalian University of Technology, Dalian 116024, China |
引用本文:
陈永君, 胡小刚, 羌建兵, 董闯. 准晶磨料的“碾抹”特性对软金属表面的平整性、硬度及耐蚀性的影响*[J]. 金属学报, 2016, 52(10): 1353-1362.
Yongjun CHEN,
Xiaogang HU,
Jianbing QIANG,
Chuang DONG.
QUASICRYSTAL ABRASIVE POLISHING ON SOFT METALS VIA A CHARACTERISTIC SMEARING WEAR MECHANISM FOR EFFICIENT SURFACE FLATTENING, HARDENING AND CORROSION ENHANCEMENT[J]. Acta Metall Sin, 2016, 52(10): 1353-1362.
[1] | Malkin S, Guo C S.Grinding Technology: Theory and Applications of Machining with Abrasives. 2nd Ed., New York: Industrial Press, 2008: 11 | [2] | Samuel L E.In: Blau P J ed., Friction, Lubrication, and Wear Technology. USA: ASM International, 1992: 352 | [3] | Qiang J B, Chen Q B, Dong C, Wang Y M, Wang Q.Chin Pat, 103242803, 2013 | [3] | (羌建兵, 陈千宝, 董闯, 王英敏, 王清. 中国专利, 103242803, 2013) | [4] | Chen Y J, Qiang J B, Dong C.Intermetallics, 2016; 68: 23 | [5] | Ledieu J, Fournée V.C R Phys, 2014; 15: 48 | [6] | Rabson D A.Prog Surf Sci, 2012; 87: 253 | [7] | Thiel P A.Annu Rev Phys Chem, 2008; 59: 129 | [8] | Musil J, Nova?k P, C?erstvy? R, Soukup Z.J Vac Sci Technol, 2010; 28A: 244 | [9] | Leyland A, Matthews A.Wear, 2000; 246: 1 | [10] | Jenks C J, Thiel P A.Langmuir, 1998; 14: 1392 | [11] | Tsai A P, Inoue A, Masumoto T.Jpn J Appl Phys, 1987; 26: L1505 | [12] | Dubois J, Kang S, Stebut J V.J Mater Sci Lett, 1991; 10: 537 | [13] | Dubois J M.Chem Soc Rev, 2012; 41: 6760 | [14] | Bloom P D, Baikerikar K, Otaigbe J U, Sheares V V.Mater Sci Eng, 2000; A294: 156 | [15] | Huttunen-Saarivirta E.J Alloys Compd, 2004; 363: 150 | [16] | Richardson R.Wear, 1967; 10: 291 | [17] | Richardson R.Wear, 1968; 11: 245 | [18] | Larsen-Basse J, Premaratne B.In: Ludema K C ed., Proc Int Conf on Wear of Materials, New York: ASME, 1983: 161 | [19] | Deuis R, Subramanian C, Yellup J.Wear, 1996; 201: 132 | [20] | Blau P J.ASM Handbook. Vol.18, 10th Ed., Ohio: ASM International, 1992: 337 | [21] | Kang S S, Dubois J M, Stebut J V.J Mater Res, 1993; 8: 2471 | [22] | K?ster U, Liu W, Liebertz H, Michel M.J Non-Cryst Solids, 1993; 153: 446 | [23] | Bauccio M.ASM Engineered Materials Reference Book. 2nd Ed., Ohio: ASM international, 1994: 280 | [24] | Marinescu I D.Handbook of Advanced Ceramics Machining. Boca Raton: CRC Press, 2006: 10 | [25] | Dong C, Perrot A, Dubois J M, Belin E. Mater Sci Forum, 1994; 150-151: 403 | [26] | Chen Q B, Wang Y B, Qiang J B, Chen H, Wang Y M, Wang Q, Dong C.Chin J Nonferrous Met, 2013; 23: 1315 | [26] | (陈千宝, 王雁斌, 羌建兵, 陈华, 王英敏, 王清, 董闯. 中国有色金属学报, 2013; 23: 1315) | [27] | Huang F, Wang J Q, Han E H, Ke W.Acta Metall Sin, 2011; 47: 7 | [27] | (黄发, 王俭秋, 韩恩厚, 柯伟. 金属学报, 2011; 47: 7) |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|