金属学报  1987, Vol. 23 Issue (2): 158-161    
  论文 本期目录 | 过刊浏览 |
合金结构钢的一种伪断口遗传
戚正风;任瑞铭
大连铁道学院;大连铁道学院
A PSEUDO-INHERITANCE OF FRACTURE OF ALLOY STRUCTURAL STEEL
QI Zhengfeng; REN Ruiming (Dalian Railway Institute) (Manuscript received 15 February; 1985; revised manuscript 23 April; 1986)
引用本文:

戚正风;任瑞铭. 合金结构钢的一种伪断口遗传[J]. 金属学报, 1987, 23(2): 158-161.
, . A PSEUDO-INHERITANCE OF FRACTURE OF ALLOY STRUCTURAL STEEL[J]. Acta Metall Sin, 1987, 23(2): 158-161.

全文: PDF(1700 KB)  
摘要: <正> 过热淬火组织以中速加热时,将得到等轴奥氏体晶粒.尽管此时观察到的奥氏体晶粒已经细化,但仍可能出现断口遗传,得到粗晶断口.这种断口遗传的机理到目前为止,还未完全弄清. 引起这种断口遗传的原因之一,是在第一次
Abstract:Such inheritance of fracture is a pseudo-inheritance of fracture if the quenching structure, overheated not too seriously, of the alloy structural steel 40CrNi underwent requenching from normal quenching temperature reheating up at medium rate. This coarse grain fracture, showing one of the priorly overheated coarse austenite grain, is, in reality, fine grain fracture along fine equiaxial austenite grain boundary formed on reheating at medium rate. So it is called the pseudo-inheritance of fracture. It seems to be not affected on the impact toughness. The origin of pseudo-inheritance of fracture has been discussed.
收稿日期: 1987-02-18     
1 戚正风,刘世程.大连铁道学院学报,1983;(1-2) :21
2 Ko T, Hanson D. J Iron Steel Inst 1950; 164: 51
3 赵坚.金属学报,1978;14:316
4 #12
5 #1
No related articles found!