Si在Al—0.35wt—%Si合金表面的非平衡偏聚 |
陈宁;余宗森 |
北京科技大学;北京科技大学材料物理系;教授;北京(100083) |
|
NON-EQUILIBRIUM SEGREGATION OF Si ON Al-0.35wt-%Si ALLOY SURFACE |
CHEN Ning; YU Zongsen (University of Science and Technology Beijing) |
引用本文:
陈宁;余宗森. Si在Al—0.35wt—%Si合金表面的非平衡偏聚[J]. 金属学报, 1992, 28(9): 63-66.
,
.
NON-EQUILIBRIUM SEGREGATION OF Si ON Al-0.35wt-%Si ALLOY SURFACE[J]. Acta Metall Sin, 1992, 28(9): 63-66.
1 Aust K T, Hanneman R E, Niessen P, Westbrook J H. Acta Metall, 1968; 16: 291 2 余宗森,陈宁.中国科学,待发表 3 Joshi A, Shastry C R, Levy M. Metall TranS, 1981; 12A: 1081 4 Basu B K, Elbaum C. Acta Metall, 1965; 13: 1117 5 Kasen M B, Polonis D H. Acta Metall. 1962; 10: 821 6 Dorherty P E, Davis R S. Acta Metall. 1959; 7: 118 7 Kasen M B, Taggart R, Polonis D H. PhilOS Mag. 1966; 13: 453 8 Tariyal B K, Ramaswami B. J Appl Phys. 1969; 40: 4822 9 Anthony T R. Acta Metall, 1970; 18: 307` |
|