第二、三代镍基单晶高温合金含Hf过渡液相连接* |
郁峥嵘1,丁贤飞2,曹腊梅3,郑运荣1,冯强1,4() |
1 北京科技大学新金属材料国家重点实验室, 北京100083 2 北京科技大学国家材料服役安全科学中心, 北京 100083 3 北京航空材料研究院先进高温结构材料重点实验室, 北京100095 4 北京科技大学高端金属材料特种熔炼与制备北京市重点实验室, 北京 100083 |
|
TRANSIENT LIQUID PHASE BONDING OF SECOND AND THIRD GERNERATION Ni-BASED SINGLE CRYSTAL SUPERALLOY WITH Hf-CONTAININGINTERLAYER ALLOY |
Zhengrong YU1,Xianfei DING2,Lamei CAO3,Yunrong ZHENG1,Qiang FENG1,4() |
1 State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing, Beijing 100083, China 2 National Centre for Materials Service Safety, University of Science and Technology Beijing, Beijing 100083, China 3 Science and Technology on Advanced High Temperature Structural Materials Laboratory, Beijing Institute of Aeronautical Materials, Beijing 100095, China 4 Beijing Key Laboratory of Special Melting and Reparation of High-End Metal Materials, University of Science and Technology Beijing, Beijing 100083, China |
引用本文:
郁峥嵘,丁贤飞,曹腊梅,郑运荣,冯强. 第二、三代镍基单晶高温合金含Hf过渡液相连接*[J]. 金属学报, 2016, 52(5): 549-560.
Zhengrong YU,
Xianfei DING,
Lamei CAO,
Yunrong ZHENG,
Qiang FENG.
TRANSIENT LIQUID PHASE BONDING OF SECOND AND THIRD GERNERATION Ni-BASED SINGLE CRYSTAL SUPERALLOY WITH Hf-CONTAININGINTERLAYER ALLOY[J]. Acta Metall Sin, 2016, 52(5): 549-560.
[1] | Pollock T M, Tin S.J Propul Power, 2006; 22: 361 | [2] | Rolls-Royce. The Jet Engine.Derby, United Kingdom: Rolls-Royce Plc, 1986: 45 | [3] | Kercher D M.US Pat, US3533712 A, 1970 | [4] | Godfrey D G, Morris M C, Menon M.US Pat, US20130195673 A1, 2013 | [5] | Finn S R, Schilling J C, Lin W W L, Dindar M, Tyler R P.US Pat, US6607358 B2, 2002 | [6] | Qu W Q, Zhang Y H.Weld Technol, 2002; 31(3): 4 | [6] | (曲文卿, 张彦华. 焊接技术, 2002; 31(3): 4) | [7] | Duvall D S, Owczarski W A, Paulonis D F.Weld J, 1974; 53: 203 | [8] | Cook G O, Sorensen C D.J Mater Sci, 2011; 46: 5305 | [9] | Tokoro K, Wikstrom N P, Ojo O A, Chaturvedi M C.Mater Sci Eng, 2008; A477: 311 | [10] | Bakhtiari R, Ekrami A, Khan T.Mater Sci Eng, 2012; A546: 291 | [11] | Li X H, Ye L, Zhong Q P, Xiong H P.J Aeronaut Mater, 2011; 31(6): 1 | [11] | (李晓红, 叶雷, 钟群鹏, 熊华平. 航空材料学报, 2011; 31(6): 1) | [12] | Lang B, Hou J B, Wu S.J Mater Eng, 2010; (10): 32 | [12] | (郎波, 侯金保, 吴松. 材料工程, 2010; (10): 32) | [13] | Li W, Jin T, Hu Z Q. Acta Metall Sin, 2008; 44: 1474 | [13] | (李文, 金涛, 胡壮麒. 金属学报, 2008; 44: 1474) | [14] | Liu J D, Jin T, Zhao N R, Wang J H, Liu J L, Sun X F.Rare Met Mater Eng, 2007; 36: 332 | [14] | (刘纪德, 金涛, 赵乃仁, 王金辉, 刘金来, 孙晓峰. 稀有金属材料与工程, 2007; 36: 332) | [15] | Jalilian F, Jahazi M, Drew R.Mater Sci Eng, 2006; A423: 269 | [16] | Pouranvari M, Ekrami A, Kokabi A H.J Alloys Compd, 2008; 461: 641 | [17] | Pouranvari M, Ekrami A, Kokabi A H.J Alloys Compd, 2009; 469: 270 | [18] | Pouranvari M, Ekrami A, Kokabi A H.Mater Sci Eng, 2013; A568: 76 | [19] | Pouranvari M, Ekrami A, Kokabi A H.J Alloys Compd, 2013; 563: 143 | [20] | Zheng Y R, Ruan Z C.Acta Metall Sin, 1990; 26: B119 | [20] | (郑运荣, 阮中慈. 金属学报, 1990; 26: B119) | [21] | Neumeier S, Dinkel M, Pyczak F, G?ken M.Mater Sci Eng, 2011;A528: 815 | [22] | Dinkel M K, Heinz P, Pyczak F, Volek A, Ott M, Affeldt E, Singer R F.In: Reed R C, Green K A, Caron P, Gabb T P, Fahrmann M G, Huron E S, Woodard S R eds., Proc Int Symp on Superalloys, Warrendale, PA, USA: TMS, 2008: 211 | [23] | Ruan Z C, Wang S C, Zheng Y R.Scr Mater, 1996; 34: 163 | [24] | Kvasnitskij V V, Kostin A M, Vorob'ev A N, Kulik S G, Nikolaenko V P.Avtom Svarka, 1999; 11: 22 | [25] | Mao W, Li X H, Zhou Y, Ye L.Trans China Weld Inst, 2011; 32(4): 91 | [25] | (毛唯, 李晓红, 周媛, 叶雷. 焊接学报, 2011; 32(4): 91) | [26] | Cao J, Song X G, Zheng Z J, Feng J C.Trans China Weld Inst, 2011; 32(7): 13 | [26] | (曹健, 宋晓国, 郑祖金, 冯吉才. 焊接学报, 2011; 32(7): 13) | [27] | Pollock T M.Mater Sci Eng, 1995; B32: 255 | [28] | Cao L M, Li X H, Chen J Y, Xue M, Zhang Y.J Mater Eng, 2011; (10): 7 | [28] | (曹腊梅, 李相辉, 陈晶阳, 薛明, 张勇. 材料工程, 2011; (10): 7) | [29] | Chen J Y, Cao L M, Xue M, Liu L J.Rare Met, 2014; 33(2): 144 | [30] | Zheng Y R, Cai Y L, Ruan Z C, Ma S W.J Aeronaut Mater, 2006; 26(3): 25 | [30] | (郑运荣, 蔡玉林, 阮中慈, 马书伟. 航空材料学报, 2006; 26(3): 25) | [31] | Ma S W, Zheng Y R.Chin J Mater Res, 2009; 10: 149 | [31] | (马书伟, 郑运荣. 材料研究学报, 2009; 10: 149) | [32] | Wilson B, Hickman J, Fuchs G.JOM, 2003; 55(3): 35 | [33] | Zhou Y, Gale W, North T.Int Mater Rev, 1995; 40: 181 | [34] | Steuer S, Singer R.Metall Mater Trans, 2013; 44A: 2226 | [35] | Li T, Wang Q Y, Wang A Q, Wen Z X, Yue Z F.Key Eng Mater, 2005; 297: 1489 | [36] | Cranck J.The Mathematics of Diffusion. 2nd Ed., Oxford: Clarendon Press, 1975: 71 | [37] | Sheng N, Liu J, Jin T, Sun X F, Hu Z Q.Metall Mater Trans, 2013; 44A: 1793 | [38] | Karunaratne M, Reed R.Acta Mater, 2003; 51: 2905 | [39] | Bergner D.Cryst Res Technol, 1972; 7: 651 | [40] | Liu J D, Jin T, Zhao N R, Wang Z H, Sun X F, Guan H R, Hu Z Q.Mater Charact, 2011; 62: 545 | [41] | Wikstrom N, Ojo O, Chaturvedi M.Mater Sci Eng, 2006; A417: 299 | [42] | Lander J, Kern H, Beach A.J Appl Phys, 1952; 23: 1305 | [43] | Bridges P J, White C H, Durber G L R. The Nimonic Alloys. Bristol, Great Britain: Edward Arnold Ltd, 1974: 33 | [44] | Walston W S, Schaeffer J C, Murphy W H.In: Kissinger R D, Deye D J, Anton D L, Cetel A D, Nathal M V, Pollock T M, Woodford D A eds., Proc Int Symp on Superalloys, Warrendale, PA, USA: TMS, 1996: 9 | [45] | Yang C C, Rollett A, Mullins W.Scr Mater, 2001; 44: 2735 |
|
|