金属学报  1998, Vol. 34 Issue (12): 1233-1242    
  论文 本期目录 | 过刊浏览 |
Au-Cu系中无序和有序相的晶格常数
谢佑卿
中南工业大学材料科学与工程系;长沙;410083
LATTICE CONSTANTS OF DISORDERED AND ORDERED PHASES IN Au-Cu SYSTEM
XIE Youqing(Department of Materials Science and Engineering; Central South University of Technology; Changsha 410083)Correspondent:XIE Youqing; professor; Tel: (0731)8879287; Fax. (O731)8826136Manuscript received 1997-11-14; in revised form 1998-02-12
全文: PDF(776 KB)  
摘要: 

依据合金特征晶体理论,固溶体中组元的原子状态分裂成若干特征原子状态,固溶体的晶格常数可由特征晶体的晶格常数相加定律、特征原子体积相加定律和特征原子状态相加定律求得。介绍了无序二元固溶体的9种晶格常数函数;确定了无序Au-Cu合金及其组元的晶格常数函数;预计了Au_3Cu,AuCu,AuCu_3和相应有序合金随成分变化的晶格常数、理论值与实验值符合较好.

关键词 Au-Cu系无序合金有序合金晶格常数原子体积    
Abstract

According to characteristic crystal theory of alloy phases, atomic state of acomponent is split into some characteristic atomic states in the solid solution. Lattice constantsof alloys may be obtained by characteristic lattice constaat additive law, characteristic atomicvolume additive law and characteristic atomic state additive law, but they are not equal in value.Nine lattice constant functions of disordered binary solid solutions are introduced. The functionssuitable for disordered An-Cu alloys and their components have been determined. Lattice constats of Au3Cu, AuCu, AuCu3 and relevant ordered alloys as a function of composition havebeen pradicated. Theoretical values are in good agreement with eXperimental values.

Key wordsAn-Cu system    disordered alloy    ordered alloy    lattice constant    atomic volume
     出版日期: 1998-12-18
基金资助:

国家自然科学基金!59671030

引用本文:

谢佑卿. Au-Cu系中无序和有序相的晶格常数[J]. 金属学报, 1998, 34(12): 1233-1242.
XIE Youqing(Department of Materials Science and Engineering; Central South University of Technology; Changsha 410083)Correspondent:XIE Youqing; professor; Tel: (0731)8879287; Fax. (O731)8826136Manuscript received 1997-11-14; in revised form 1998-02-12. LATTICE CONSTANTS OF DISORDERED AND ORDERED PHASES IN Au-Cu SYSTEM. Acta Metall Sin, 1998, 34(12): 1233-1242.

链接本文:

http://www.ams.org.cn/CN/      或      http://www.ams.org.cn/CN/Y1998/V34/I12/1233

1谢 佑卿,马柳莺.中南矿冶学院学报,1985;3:1(Xie Y Q, Ma L Y.J Central-South Inst Min Metall,1985;3: 1)2 Vegard L. Z PhyS, 1921; 5: 173 Zen E-an. Am Mineral,1956; 41: 5234谢佑卿,马柳莺中南矿冶学院学报,1985;1:1(Xie Y Q, Ma L Y J Cent South Iust Min Metall, 1985; 1: 1)5 Lupis C H P, Elliott J F. Acta Metall, 1967; 15: 2656 Xie Y Q. Acta Metall Matet 1994; 11:37057谢佑卿,张晓东,陈嘉砚中国科学,1996;E26:224(Xie Y, Zhang X D, Chen J Y. Sci Chin, 1996; E39: 394)8 谢佑卿.中国科学,19972:E27:488(Xie Y Q.SCi Chin,1998; E41:146)9 Okamoto H, Chakrabarti D J, Laughlin D E, Massalski T B Bull Alloy Phase Diagrams.1987; 8: 45410谢佑卿,张晓东金属学报, 1994; A30: 531(Xie Y Q, Zhang X D. Acta Metall Sin, 1994; A30: 531)11Pearson W B.Handbook of Lattice Spacings and Structure of Metals and alloys.London:Pergamon,1958:41112 Johannsson C H, Linde J O Ann Phys, 1936 25: 113 Okamura K, Iwasaki H, Ogawa S j Phys Soc jpn, 1968; 24: 56914 Flinn P A, McManus G M, Rayne J A J Phys Chem Solids, 1960; 15: 189
[1] 田素贵,王欣,谢君,刘臣,郭忠革,刘姣,孙文儒. GH4169G合金热处理期间的相转变特征与机理分析[J]. 金属学报, 2013, 49(7): 845-852.
[2] 王有道 吴尔冬 王苏程 李武会. 镍基合金DD10中γ/γ'晶格错配度厚度效应的X射线衍射分析[J]. 金属学报, 2011, 47(11): 1418-1425.
[3] 谢佑卿. Cu-Ni合金组元的偏原子体积与平均原子体积的关系[J]. 金属学报, 1998, 34(12): 1243-1248.
[4] 王建强;曾梅光;晁月盛;张宝金;胡壮麒. 快速凝固Al-Fe-V-Si合金微结构Mossbauer谱研究[J]. 金属学报, 1997, 33(4): 359-363.
[5] 卢柯;刘学东;张皓月;胡壮麒. 纯镍纳米晶体的晶格膨胀[J]. 金属学报, 1995, 31(2): 74-78.
[6] 林均品;褚武扬;肖纪美. B_2型Fe_3Al金属间化合物的应力腐蚀和氢致开裂[J]. 金属学报, 1994, 30(2): 85-90.
[7] 谢佑卿;张晓东. Au-Cu合金的微观结构和性质[J]. 金属学报, 1994, 30(12): 531-539.
[8] 虞炳西;高树浚. 氢对Ti合金的Debye温度和晶格常数的影响[J]. 金属学报, 1990, 26(6): 29-33.