金属晶粒自身细化 |
边秀房;邹新国;刘广荣;刘相法;马家骥 |
山东工业大学;济南;250061;山东工业大学;济南;250061;山东工业大学;济南;250061;山东工业大学;济南;250061;山东工业大学;济南;250061 |
|
SELF GRAIN REFINEMENT OF METALS |
BIAN Xiufang; ZHOU Xinguo; LIU Guangrong; LIU Xianfa; MA Jiaji (ShandongUniversity ofTechnology; Ji'nan; 250061) |
引用本文:
边秀房;邹新国;刘广荣;刘相法;马家骥. 金属晶粒自身细化[J]. 金属学报, 1997, 33(6): 602-608.
,
,
,
,
.
SELF GRAIN REFINEMENT OF METALS[J]. Acta Metall Sin, 1997, 33(6): 602-608.
1Mitra P K,Bhattacharya I N.Trans India Inst Met,1986;39(2):150 2著,王永海,张发明,高革译.变形铝合金的细 化处理北京:冶金工业出版社,1988:201 3Flemings M C.Solidification processing,New York:Mc Graw Hill,1974:155 4胡汉起.金属凝固.北京:冶金工业出版社,1985:294 5Hadlet D. Solidification processing,London: The Institute of Metals, 1987: 141 6Spittle J A, Sadlis. Cast Metals, 1995; 7: 247 7Mondolfa L F. Solidification processing, London: The Institute ofMetal, 1987: 133 8 BanerjiA,Reif w.J Mater Sci,1994;29:1958 9安阁英.铸件形成理论.北京:机械工业出版社,1990:147 10铝及铝合金加工制品低倍组织检验方法,GB3247—82 11 Matyia H,Giessen B C,Grant N J.J Inst Met,1968;96:30 12Pearson J,Birch M E J, Haldet D. Solidification Technology in the Foundry and Casthouse, London:Mid—Count Press, 1980: 70 13Ponies P S, de Galiza J A, Robert M H, Cupini N L. Solidification Technology in the Foundry andCasthouse, London: Mid-County Press, 1980: 74 14王广厚.物理学进展,1994;14:121 15蔡英文,范新会,李建国,傅恒志.西北工业大学学报,1996;14:323 16刘相法,边秀房,李辉,马家骥.金属学报,1996;32:149 17 1966:562 18 1940; 10: 942 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|