金属学报  1997, Vol. 33 Issue (6): 577-582    
  论文 本期目录 | 过刊浏览 | 高级检索 |
Al—Li单晶体中锯齿流变行为的影响因素
田宝辉;李焕喜;张永刚;陈昌麒
北京航空材料研究院;北京;100095;北京航空航天大学;北京;100083;北京航空航天大学;北京;100083;北京航空航天大学;北京;100083
INFLUENCING FACTORS OF SERRATED FLOW IN Al-Li SINGLE CRYSTALS
Tian Baohui (Beijing Institute of Aeronautical Materials; Beijing 100095); Li HuanxiZhang Yonggang;Chen Changqi(Beijing University of Aeronautics and Astronautics;Beijing 100083)
下载:  PDF(587KB) 
输出:  BibTeX | EndNote (RIS)      
摘要 Al-Li单晶体中锯齿流变的产生与δ',粒子被切割的过程有关锯齿产生的临界应变随温度、应变速率和时效状态而变化时效状态和加载的晶体位向对锯齿的平均经历时间和应力幅度有影响
服务
把本文推荐给朋友
加入引用管理器
E-mail Alert
RSS
作者相关文章
田宝辉
李焕喜
张永刚
陈昌麒
关键词:  锯齿流变(PLC效应)  Al-Li合金  单晶体    
Abstract: Occurrence of serrated flow in Al-Li single crystals is related to the shearingof δ' particles. Critical strain varies with temperature, strain rate and aging state. The agingconditions and crystal orientations of the loading axes have some effects on the time periodwithin one cycle of serration and stress amplitude of serration.
Key words:  serrated flow (PLC) effect    Al-Li alloy    single crystal
收稿日期:  1997-06-18      修回日期:  1997-06-18           出版日期:  1997-06-18      发布日期:  1997-06-18      期的出版日期:  1997-06-18
基金资助: 国家自然科学基金;;航空基金资助
引用本文:    
田宝辉;李焕喜;张永刚;陈昌麒. Al—Li单晶体中锯齿流变行为的影响因素[J]. 金属学报, 1997, 33(6): 577-582.
Tian Baohui (Beijing Institute of Aeronautical Materials; Beijing 100095); Li HuanxiZhang Yonggang;Chen Changqi(Beijing University of Aeronautics and Astronautics;Beijing 100083). INFLUENCING FACTORS OF SERRATED FLOW IN Al-Li SINGLE CRYSTALS. Acta Metall Sin, 1997, 33(6): 577-582.
链接本文:  
http://www.ams.org.cn/CN/  或          http://www.ams.org.cn/CN/Y1997/V33/I6/577
1Wert J A,Wycliffe P A.Scr Metall Mater,1985;19:463
2 Gregson P J.McDarmaid D S,Hunt E.Mater Sci Technol,1988;4:713
3Tamura M, Mori T,Nakamura T. Trans JIM, 1973;14: 355
4 Zambo S J,Wert J A.Scr Melall Mater,1993;29:1523
5 Huang J C,Gray G T.Scr Metall Mater,1990;24:85
6 Deladosse D,Lapasset G,Kubin L P.Scr Metall Mater,1993;28:1379
7 Ilic N,Drobniak Dj,Radmilovic V,Jovanovic M T,Markovic D.Scr Metll Maler,1996;34:1123
8 Diego N, Rio J del, Segers D, Dorikens—Vanpraet L, Dorikens M. Phy Rev(B), 1993; 48: 6781
9King J E, You C Y, Knott J F. Acta Metall, 1981:29: 1553
10 Cottrell A H.Dislocation and Plastic Flow in Crysals,Clarendon,Oxford,1953:136
11 Wood J,McCormick P G.Acta Metall ,1971;19:463
12 Bchnood N, Evans J T Acta Metall, 1989; 37: 687
13 Evans J T.Scr Metall Mater,1987;21:435
14 Miuya Y,Matsui A,Furukawa M,Nemoto M.In:Baker C,Gregson D J, Harris S T,Peel C T eds,Aluminum—Lithium Alloys III, London:Inst of Metals,1986:427
15 Brechet Y,Estrin Y.Scr Metall Mater,1994:31:185
16 Fujita H, Tanata T Acta Metall, 1982; 25: 793=
[1] 李劲风,刘丹阳,郑子樵,陈永来,张绪虎. Er微合金化对2055 Al-Li合金微观组织及力学性能的影响*[J]. 金属学报, 2016, 52(7): 821-830.
[2] 郭巍巍,齐成军,李小武. 共轭和临界双滑移取向Cu单晶体疲劳位错结构的热稳定性研究*[J]. 金属学报, 2016, 52(6): 761-768.
[3] 刘奋军, 傅莉, 张纹源, 孟强, 董春林, 栾国红. 2099-T83/2060-T8异质Al-Li合金搅拌摩擦焊搭接界面结构与力学性能[J]. 金属学报, 2015, 51(3): 281-288.
[4] 王晓钢,姜潮,韩旭. Ni单晶体塑性应变的非均匀性与加工硬化*[J]. 金属学报, 2015, 51(12): 1457-1464.
[5] 郭巍巍,齐成军,李小武. 一个共面双滑移取向Cu单晶体疲劳位错结构的热稳定性研究[J]. 金属学报, 2013, 49(1): 107-114.
[6] 王东 董春林 肖伯律 高崇 何淼 栾国红 马宗义. 焊接参数对AlCuLi合金搅拌摩擦焊接头微观结构和力学性能的影响[J]. 金属学报, 2012, 48(9): 1109-1115.
[7] 李小武 曹昕明 马超群. 含富Cr沉淀颗粒Fe--Cr合金单晶体的疲劳变形特征[J]. 金属学报, 2009, 45(7): 801-807.
[8] 刘江涛 王中光 尚建库. [110]和[112]取向β-Sn单晶体的形变行为[J]. 金属学报, 2008, 44(12): 1409-1414.
[9] 朱荣; 李守新; 李勇; 李明扬; 晁月盛 . Cu单晶体驻留滑移带的形成与消失[J]. 金属学报, 2004, 40(5): 467-470 .
[10] 杨继红; 贾维平; 李守新 . [013]取向Cu单晶体在NaCl水溶液中腐蚀疲劳位错结构的观察[J]. 金属学报, 2004, 40(1): 99-102 .
[11] 李劲风; 张昭; 曹发和; 程英亮; 张鉴清; 曹楚南 . Al-Li合金在EXCO溶液中腐蚀的电化学阻抗研究[J]. 金属学报, 2003, 39(4): 426-430 .
[12] 李晓玲; 陈铮; 刘晓光; 刘兵 . Al-Li合金中δ'相沉淀过程原子图像的计算机模拟[J]. 金属学报, 2002, 38(5): 458-462 .
[13] 刘志义; 刘冰 . 脉冲电流对2091Al-Li合金超塑变形机理的影响[J]. 金属学报, 2000, 36(9): 944-951 .
[14] 吴细毛; 王中光; 李广义 . [112]-Cu-7Al单晶体循环形变行为Ⅰ.应变突发行为[J]. 金属学报, 1999, 35(8): 789-792 .
[15] 吴细毛; 王中光; 李广义 . [112]Cu-7Al单晶体循环形变行为 Ⅱ.循环形变特征[J]. 金属学报, 1999, 35(8): 793-795 .
No Suggested Reading articles found!
Viewed
Full text


Abstract

Cited

  Shared   
  Discussed