Please wait a minute...
金属学报  1993, Vol. 29 Issue (1): 11-15    
  论文 本期目录 | 过刊浏览 |
立方系完整ODF测算的改进
赵宏;王福;徐家桢;梁志德
东北工学院;东北工学院;东北工学院;东北工学院
IMPROVEMENT ON COMPLETE ODF DETERMINATION OF CUBIC SYSTEM MATERIALS
ZHAO Hong;WANG Fu;XU Jiazhen;LIANG Zhide Department of Materials Science and Engineering; Northeast University of Technology; Shenyang
全文: PDF(320 KB)  
摘要: 本文通过对具有宏观统计对称立方晶系材料用最大熵法测算完整ODF的研究,提出了适于微计算机用的测算方法,并在PANAFACOM—U1200机上建立了相应的软件系统。作者用冷轧磷钢板材的织构对方法(如系统)进行了校验,结果表明,该法是可靠、实用的
关键词 最大熵法完整的ODF    
Abstract:Suitable method and relevant software for micro-computer were developedon the basis of revision of the maximum entropy method (MEM) for determining the com-plete ODF of macrostatistical symmetrical cubic system materials. The method was verifiedby testing the complete ODF of the cold-rolled phosphoratic steel sheet, and seemed to be re-liable and practicable.
Key wordsmaximum entropy method    complete ODF    cubic system material
收稿日期: 1993-01-18      出版日期: 1993-01-18
基金资助:国家教委博士点基金

引用本文:

赵宏;王福;徐家桢;梁志德. 立方系完整ODF测算的改进[J]. 金属学报, 1993, 29(1): 11-15.
ZHAO Hong;WANG Fu;XU Jiazhen;LIANG Zhide Department of Materials Science and Engineering; Northeast University of Technology; Shenyang. IMPROVEMENT ON COMPLETE ODF DETERMINATION OF CUBIC SYSTEM MATERIALS. Acta Metall Sin, 1993, 29(1): 11-15.

链接本文:

http://www.ams.org.cn/CN/      或      http://www.ams.org.cn/CN/Y1993/V29/I1/11

1 Bunge H-J, Esling C. J Appl Crystallogr, 1981; 14: 2532 Bunge H-J, Esling C. Proc 6th Int Conf on Textures of Materials, Vol. Ⅱ, Tokyo: Iron Steel Inst Japan, 1981: 13593 Pospiech J, Luecke, K, Jura J. proc 6th Int Conf on Textures of Materials, Vol. Ⅱ, Tokyo: Iron Steel Inst Japan, 1981: 13904 Van Houtte P. Textures Microstruct, 1983; 6: 15 Wang Fu, Xu Jiazheng, Liang Zhide. In: Kallend J S, Gottstein G eds. Proc 8th Int Conf on Textures of Materials, New York: Metallurgical Society, 1988: 1116 Wang Fu, Xu Jiazheng, Liang Zhide. Textures Microstruct, 1989; 10: 2177 Wang Fu, Xu Jiazheng, Liang Zhide. Textures Microsturct, 1992; 1991: 558 陈礼清.东北工学院硕士学位论文,19919 梁志德,徐家恢,王福.织构的三维取向分析技术,沈阳:东北工学院出版社,198610 Hu H.金属学报,1980;16:121
[1] 王大鹏 王大志 武宝林 左良 王福 梁志德. 粒子群算法对织构分析改进最大熵法的改进[J]. 金属学报, 2009, 45(1): 63-66.