金属学报  1987, Vol. 23 Issue (2): 156-157    
  论文 本期目录 | 过刊浏览 |
35钢低周扭转应变疲劳的研究
赵廷仕;刘敦康;纪惠君
华中工学院;华中工学院;华中工学院
LOW CYCLE FATIGUE OF STEEL 35 UNDER TORSIONAL STRAIN
ZHAO Tingshi; LIU Dunkang; JI Huijun(Huazhong University of Science and Technology; Wuhan) (Manuscript received 31 December; 1984; revised manuscript 10 July; 1986)
全文: PDF(174 KB)  
摘要: <正> 一、循环扭转下材料的特性 35钢材料一次扭转断裂和反复多次断裂,两者的本构关系不同.实验在岛津DCS25t试验机上进行,频率为3—5cyc/min.试样机械加工成直径12mm、标距长150mm的圆柱. 35钢为热轧一般质量的
Abstract:Studies were made of the material performance of steel 35 under low cycle torsion as well as the relationship of the low cycle torsional fatigue life together with the torsional strain amplitude and fatigue energy under torsion strain. The feature of the fatigue failure of the steel under low cycle torsion was also discussed.
收稿日期: 1987-02-18      出版日期: 1987-02-18

引用本文:

赵廷仕;刘敦康;纪惠君. 35钢低周扭转应变疲劳的研究[J]. 金属学报, 1987, 23(2): 156-157.
ZHAO Tingshi; LIU Dunkang; JI Huijun(Huazhong University of Science and Technology; Wuhan) (Manuscript received 31 December; 1984; revised manuscript 10 July; 1986). LOW CYCLE FATIGUE OF STEEL 35 UNDER TORSIONAL STRAIN. Acta Metall Sin, 1987, 23(2): 156-157.

链接本文:

http://www.ams.org.cn/CN/      或      http://www.ams.org.cn/CN/Y1987/V23/I2/156

1 徐灏,疲劳强度设计.机械工业出版社,1981,277-2882 Hertzberg R W.工程材料的变形与断裂力学,王克仁等译.1982,4953 谢济洲.机械强度,1980;(11) :75-83
No related articles found!