AN ENGINEERING METHOD FOR CALCULATION OF BOTH THEORETICAL COKE RATE AND EFFECTS OF DIFFERENT FACTORS ON COKE RATE
YANG YUNG-YI(Peking Institute of Ferrous Metallurgy)
全文: PDF(1033 KB)  
摘要: 理論焦比是指在一定原料和风溫条件下渗碳、发热和还原所需的焦炭;現有各种計算方法的缺点;以风口热函減去炉頂煤气热函作为唯一热量收入的热平衡計算方法,以物料平衡和热平衡結合为基础,利用偏微分找出的計算各种因素对焦比影响的方法。
Abstract:Theoretical coke rate means the necessary amount of coke to satisfy the thermal and chemical requirements under given conditions of raw materials, blast temperature, etc. The newly proposed method is characterized by combination of material and heat balance into one equation, and by that, the only thermal income is the heat of combustion before the tuyere with subtraction of heat carried away by the hot top gas. With this thermal balance, the necessary tuyere carbon is found. By adding to this carbon the solution carbon in pig iron and direct reduction carbon, the total carbon is finally obtained.By partial differentiation, a convenient and practically accurate method is derived for calculating effects of different factors on coke rate. Calculations for some Chinese and Japanese blast furnaces are given to show how this method might be used to examine operational efficiency, to calculate effects on coke rate of new technology like fuel injections through tuyere, and used for design purposes. Comparisons of this method with others like that of Runm and Pavlov are briefly given.
收稿日期: 1964-04-18      出版日期: 1964-04-18

引用本文:

杨永宜. 理论焦比和各种因素对焦比影响的工程计算方法[J]. 金属学报, 1964, 7(4): 348-362.
YANG YUNG-YI(Peking Institute of Ferrous Metallurgy). AN ENGINEERING METHOD FOR CALCULATION OF BOTH THEORETICAL COKE RATE AND EFFECTS OF DIFFERENT FACTORS ON COKE RATE. Acta Metall Sin, 1964, 7(4): 348-362.

链接本文:

http://www.ams.org.cn/CN/      或      http://www.ams.org.cn/CN/Y1964/V7/I4/348

[1] #12
[2] #12
[3] #12
[4] #12
[5] #12
[6] 堺千代次·○新实稔生:铁钢,1961,27,234.
[7] 李道昭、李公达:中国金属学会学术論文集,(炼铁文集) 1961年,121頁。
[8] 馬汉湼克,H.:苏联拉姆高炉配料計算方法,(重工业出版社,1953年),85-88頁.
[9] 胡嘉龙、杨永宜:石钢二、三高炉当前焦比的計算分析.
[10] #12
No related articles found!