填料形状对Fe@Ag核壳复合粒子的电磁特性的影响 |
赵素玲1,2,陈晶1,2,王一龙1,3 |
1. 武汉理工大学材料复合新技术国家重点实验室, 武汉 430070
2. 武汉理工大学材料研究与测试中心, 武汉 430070
3. 武汉理工大学理学院, 武汉 430070 |
|
INFLUENCE OF THE SHAPE OF SHIELDING FILLERS ON ELECTROMAGNETIC PROPERTIES OF Fe@Ag CORE–SHELL COMPOSITE PARTICLES |
ZHAO Suling 1,2, CHEN Jing 1,2, WANG Yilong 1,3 |
1. State Key Laboratory of Advanced Technology for Materials Synthesis and Processing, Wuhan University of Technology, Wuhan 430070
2. Center for Material Research and Testing, Wuhan University of Technology, Wuhan 430070
3. School of Sciences, Wuhan University of Technology, Wuhan 430070 |
引用本文:
赵素玲 陈晶 王一龙. 填料形状对Fe@Ag核壳复合粒子的电磁特性的影响[J]. 金属学报, 2012, 48(8): 977-982.
,
,
.
INFLUENCE OF THE SHAPE OF SHIELDING FILLERS ON ELECTROMAGNETIC PROPERTIES OF Fe@Ag CORE–SHELL COMPOSITE PARTICLES[J]. Acta Metall Sin, 2012, 48(8): 977-982.
[1] Wang Y L, Zhang Q X, Shao H M, Guan J G. Chin J Struct Chem, 2010; 29: 555[2] Tong G X, Guan J G, Fan X A, Wang W, Li W. Acta Metall Sin, 2008; 44: 867(童国秀, 官建国, 樊希安, 王维, 李维. 金属学报, 2008; 44: 867)[3] Tong G X, Guan J G, Zhang W Y, Zhang W, Wang W, Dong D M. Acta Metall Sin, 2008; 44: 1001(童国秀, 官建国, 张五一, 张巍, 王 维, 董德明. 金属学报, 2008; 44: 1001)[4] Han E G, Kim E A, Oh K W. Synth Met, 2001; 123: 469[5] Yuen S M, Ma C C M, Chuang C Y, Yu K C, Wu S Y, Yang C C, Wei M H. Compos Sci Technol, 2008; 68: 963[6] Deng H, Skipa T, Bilotti E, Zhang R, Lellinger D, Mezzol L, Fu Q, Alig I, Peijs T. Adv Funct Mater, 2010; 20: 1424[7] Wang Y L, Li W, Zhang Q X, Wang W, Guan J G. Chem J Chin Univ, 2010; 31: 1934(王一龙, 李维, 章桥新, 王维, 官建国. 高等学校化学学报, 2010; 31: 1934)[8] Cao X G, Zhang H Y. J Mater Eng, 2007; 8: 69(曹晓国, 张海燕. 材料工程, 2007; 8: 69)[9] Wu L B, Gao Y L, Li Y H. Design on Electromagnetic Compatibility of Modern Electronic System. Bejing: Defence Industry Press, 2004: 27(吴良斌, 高玉良, 李延辉. 现代电子系统的电磁兼容设计. 北京: 国防工业出版社, 2004: 27)[10] Jiang H J, Moon K S, Li Y, Wong C P. Chem Mater, 2006; 18: 2969[11] Zhang Q X, Yang L N, Zhang J M, Guan J G, Wang Y L. J Chin Ceram Soc, 2007; 35: 987(章桥新, 杨丽宁, 张佳明, 官建国, 王一龙. 硅酸盐学报, 2007; 35: 987)[12] Ye L L, Lai Z H, Liu J, Tholen A. IEEE Trans Electron Pack, 1999; 22: 299[13] Chiang H W, Chung C L, Chen L C. J Adhes Sci Technol, 2005; 19: 565[14] Walser R M, Win W. IEEE Trans Magn, 1998; 34: 1390[15] Walser R M, Kang W. IEEE Trans Magn, 1998; 34: 1144[16] Ge F D, Zhu J, Chen L M. Chin J Electron, 1996; 24(6): 82(葛副鼎, 朱静, 陈利民. 电子学报, 1996; 24(6): 82)[17] Ge F D, Zhu J, Chen L M. Aero Mater Technol, 1996; (5): 42(葛副鼎, 朱静, 陈利民. 宇航材料工艺, 1996; (5): 42)[18] Zhou J, Wang W, Sun Z G, Guan J G. Acta Metall Sin, 2010; 46: 967(周静, 王维, 孙志刚, 官建国. 金属学报, 2010; 46: 967)[19] Zhao S L, Chen J, Wang Y L, Sun Z G, Guan J G. J Inorg Mater, 2010; 25: 1180(赵素玲, 陈晶, 王一龙, 孙志刚, 官建国. 无机材料学报, 2010; 25: 1180)[20] Li ZW, Chen L, Ong C K, Yang Z. J Mater Sci, 2005; 40: 719[21] Tong G X, Wang W, Guan J G, Zhang Q J. J Inorg Mater, 2006; 21: 1461(童国秀, 王维, 官建国, 张清杰. 无机材料学报, 2006; 21: 1461)[22] Cho H S, Kim A S, Kim S M, Namgung J, Kim M C, Lee G A. Phys Status Solidi, 2004; 201A: 1942[23] Dong D M, Guan J G,Wang W, Li W, Zhou J. Acta Metall Sin, 2009; 45: 1141(董德明, 官建国, 王维, 李 维, 周静. 金属学报, 2009; 45: 1141)[24] Xie J L, Liang B L, Deng L J. Funct Mater, 2008; 39: 41(谢建良, 梁波浪, 邓龙江. 功能材料, 2008; 39: 41)[25] Ruschau G R, Yashikaw A S, Newnham R E. J Appl Phys, 1992; 72: 953 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|