Al-12.7Si合金表面强烈塑性变形诱发的纳米化 |
刘刚1,严文聪1,于福晓2,赵刚3,赵骧2,左良1 |
1. 东北大学研究院, 沈阳 110004
2. 东北大学材料电磁过程研究教育部重点实验室, 沈阳 110819
3. 东北大学材料各向异性与织构教育部重点实验室, 沈阳 110819 |
|
NANOCRYSTALLIZATION OF Al–12.7Si ALLOY INDUCED BY SURFACE INTENSE PLASTIC DEFORMATION |
LIU Gang 1, YAN Wencong 1, YU Fuxiao 2, ZHAO Gang 3, ZHAO Xiang 2, ZUO Liang 1 |
1. Research Academy, Northeastern University, Shenyang 110004
2. Key Laboratory of Electromagnetic Processing of Materials (Ministry of Education), Northeastern University, Shenyang 110819
3. Key Laboratory for Anisotropy and Texture of Materials (Ministry of Education), Northeastern University, Shenyang 110819 |
引用本文:
刘刚 严文聪 于福晓 赵刚 赵骧 左良. Al-12.7Si合金表面强烈塑性变形诱发的纳米化[J]. 金属学报, 2011, 47(6): 649-654.
,
,
,
,
,
.
NANOCRYSTALLIZATION OF Al–12.7Si ALLOY INDUCED BY SURFACE INTENSE PLASTIC DEFORMATION[J]. Acta Metall Sin, 2011, 47(6): 649-654.
[1] Lu K, Lu J. Mater Sci Eng, 2004; A375–377: 38[2] Wu X, Tao N, Hong Y, Xu B, Lu J, Lu K. Acta Mater, 2002; 50: 2075[3] Wang K, Tao N R, Liu G, Lu J, Lu K. Acta Mater, 2006; 54: 5281[4] Zhu K Y, Vassel A, Brisset F, Lu K, Lu J. Acta Mater, 2004; 52: 4101[5] Sun Q, Shi Y N, Zhng X, Lu K. Acta Mater, 2007; 55: 975[6] Wu X, Tao N, Hong Y, Liu G, Xu B, Lu J, Lu K. Acta Mater, 2005; 53: 681[7] Tao N R, Wang Z B, Tong W P, Sui M L, Lu J, Lu K. Acta Mater, 2002; 50: 4603[8] Zhang H W, Hei Z K, Liu G, Lu J, Lu K. Acta Mater, 2003; 51: 1871[9] L¨u A Q, Liu G, Liu C M. Acta Metall Sin, 2004; 40: 943(吕爱强, 刘 刚, 刘春明. 金属学报, 2004; 40: 943)[10] Wang Z B, Tao N R, Li S, Wang W, Liu G, Lu J, Lu K. Mater Sci Eng, 2003; A352: 144[11] Ba D M, Ma S N, Meng F J, Li C Q. Surf Coat Technol, 2007; 202: 254[12] Zhang Y S, Wang K, Han Z, Liu G. Wear, 2007; 262: 1463[13] Wang T, Wang D P, Liu G, Gong B M, Song N S. Appl Surf Sci, 2008; 255: 1824[14] Wei Y H, Liu B S, Hou L F, Xu B S, Liu G. J Alloy Compd, 2008; 452: 336[15] Zhou L, Liu G, Ma X L, Lu K. Acta Mater, 2008; 56: 78 |
|