调质处理对G520钢焊接接头组织及性能的影响 |
张敏(),贾芳,程康康,李洁,许帅,仝雄伟 |
西安理工大学材料科学与工程学院 西安 710048 |
|
Influence of Quenching and Tempering on Microstructure and Properties of Welded Joints of G520 Martensitic Steel |
ZHANG Min(),JIA Fang,CHENG Kangkang,LI Jie,XU Shuai,TONG Xiongwei |
School of Materials Science and Engineering, Xi’an University of Technology, Xi’an 710048, China |
引用本文:
张敏,贾芳,程康康,李洁,许帅,仝雄伟. 调质处理对G520钢焊接接头组织及性能的影响[J]. 金属学报, 2019, 55(11): 1379-1387.
Min ZHANG,
Fang JIA,
Kangkang CHENG,
Jie LI,
Shuai XU,
Xiongwei TONG.
Influence of Quenching and Tempering on Microstructure and Properties of Welded Joints of G520 Martensitic Steel[J]. Acta Metall Sin, 2019, 55(11): 1379-1387.
[1] | FanJ L, GuoX L, WuC W, et al. Influence of heat treatments on mechanical behavior of FV520B steel [J]. Exp. Tech., 2015, 39: 55 | [2] | ZhouQ Q, ZhaiY C. Aging process optimization for a high strength and toughness of FV520B martensitic steel [J]. Acta Metall. Sin., 2009, 45: 1249 | [2] | 周倩青, 翟玉春. 高强高韧FV520B马氏体钢的时效工艺优化 [J]. 金属学报, 2009, 45: 1249 | [3] | XuW B, ShiW, ZhangX. Microstructural transformation of martensite precipitation hardening stainless steel during aging process [J]. Trans. Mater. Heat Treat., 2013, 34(Suppl.2: 139 | [3] | 许文博, 石 伟, 张 欣. 马氏体型沉淀硬化不锈钢时效过程的组织转变 [J]. 材料热处理学报, 2013, 34(增刊2): 139 | [4] | NiuJ, DongJ M, XueJ. Precipitation-hardening and toughness of precipitation-hardening stainless steel FV520(B) [J]. Mater. Mech. Eng., 2007, 43(12): 78 | [4] | 牛 靖, 董俊明, 薛 锦. 沉淀硬化不锈钢FV520(B)的析出硬化及韧性 [J]. 机械工程学报, 2007, 43(12): 78 | [5] | ZhangM, WangW Q, WangP F, et al. Fatigue behavior and mechanism of FV520B in very high cycle regime [J]. Strength Fract. Complex., 2015, 9: 161 | [6] | ZhaoQ C, WangJ L, ZhangY L, et al. Fatigue behavior and fatigue life for FV520B-I at different loading frequencis [J]. Mater. Rev., 2018, 32: 2837 | [6] | 赵清晨, 王金龙, 张元良等. 不同加载频率下FV520B-I的疲劳行为与疲劳寿命 [J]. 材料导报, 2018, 32: 2837 | [7] | XiangL H, PanJ Y, ChenS Y, et al. Experimental investigation on the stress corrosion cracking of FV520B welded joint in natural gas environment with ECP and SSRT [J]. Eng. Fract. Mech., 2018, 200: 166. | [8] | XiangL H, PanJ Y, ChenS Y. Analysis on the stress corrosion crack inception based on pit shape and size of the FV520B tensile specimen [J]. Results Phys., 2018, 9: 463 | [9] | AmreiM M, MonajatiH, ThibaultD, et al. Effects of various post-weld heat treatments on austenite and carbide formation in a 13Cr4Ni steel multipass weld [J]. Metallogr. Microstruct. Anal., 2016, 5: 50 | [10] | GaoH, SongY Y, ZhaoM J, et al. Effects of tempering on the microstructure and mechanical property of electron beam welding joint of 9Cr2WVTa steel [J]. Acta Metall. Sin., 2014, 50: 1429 | [10] | 高 恒, 宋元元, 赵明久等. 回火对9Cr2WVTa钢电子束焊接接头组织和力学性能的影响 [J]. 金属学报, 2014, 50: 1429 | [11] | JorgeJ C F, MonteiroJ L D, GomesA J C, et al. Influence of welding procedure and PWHT on HSLA steel weld metals [J]. J. Mater. Res. Technol., 2019, 8: 561 | [12] | XuK C, WangH Q, GaiJ F. Draught Fan Manual [M]. 2nd Ed., Beijing: Mechanical Industry Stress, 2011: 113 | [12] | 续魁昌, 王洪强, 盖京方. 风机手册 [M]. 第2版,北京: 机械工业出版社, 2011: 113 | [13] | LiX L, WangZ D. Effect of one step Q&P process on microstructure and mechanical properties of a dual martensite steel [J]. Acta Metall. Sin., 2015, 51: 534 | [13] | 李小琳, 王昭东. 一步Q&P工艺对双马氏体钢微观组织与力学性能的影响 [J]. 金属学报, 2015, 51: 534 | [14] | AmreiM M, VerremanY, BridierF, et al. Microstructure characterization of single and multipass 13Cr4Ni steel welded joints [J]. Metallogr. Microstruct. Anal., 2015, 4: 207 | [15] | WangX N, ChenX M, SunQ, et al. Formation mechanism of δ-ferrite and metallurgy reaction in molten pool during press-hardened steel laser welding [J]. Mater. Lett., 2017, 206: 143 | [16] | HuX Q, XiaoN M, LuoX H, et al. Effects of δ-ferrite on the microstructure and mechanical properties in a tungsten-alloyed 10%Cr ultra-supercritical steel [J]. Acta Metall. Sin., 2009, 45: 553 | [16] | 胡小强, 肖纳敏, 罗兴宏等. 含W型10%Cr超超临界钢中δ-铁素体的微观结构及其对力学性能的影响 [J]. 金属学报, 2009, 45: 553 | [17] | XuB S, FangJ X, DongS Y, et al. Heat-affected zone microstructure evolution and its effects on mechanical properties for laser cladding stainless FV520B steel [J]. Acta Metall. Sin., 2016, 52: 1 | [17] | 徐滨士, 方金祥, 董世运等. FV520B不锈钢激光熔覆热影响区组织演变及其对力学性能的影响 [J]. 金属学报, 2016, 52: 1 | [18] | XiaoF R. Influence of intermediate treatment on microstructure and properties of stainless steel FV520(B) [J]. Trans. Met. Heat Treat., 1999, 20(4): 35 | [18] | 肖福仁. 调整处理对 FV520(B)不锈钢组织与性能的影响 [J]. 金属热处理学报, 1999, 20(4): 35 | [19] | LiuY R, YeD, YongQ L, et al. Effect of heat treatment on microstructure and property of Cr13 super martensitic stainless steel [J]. J. Iron Steel Res. Int., 2011, 18: 60 | [20] | CuiZ Q, QinY C. Metallography and Heat Treatment [M]. 2nd Ed., Beijing: Mechanical Industry Stress, 2007: 252 | [20] | 崔忠圻, 覃耀春. 金属学与热处理 [M]. 第2版,北京: 机械工业出版社, 2007: 252 | [21] | SongY Y, PingD H, YinF X, et al. Microstructural evolution and low temperature impact toughness of a Fe-13%Cr-4%Ni-Mo martensitic stainless steel [J]. Mater. Sci. Eng., 2010, A527: 614 | [22] | ParkE S, YooD K, SungJ H, et al. Formation of reversed austenite during tempering of 14Cr-7Ni-0.3Nb-0.7Mo-0.03C super martensitic stainless steel [J]. Met. Mater. Int., 2004, 10: 521 | [23] | SongY Y, LiX Y, RongL J, et al. Formation of the reversed austenite during intercritical tempering in a Fe-13%Cr-4%Ni-Mo martensitic stainless steel [J]. Mater. Lett., 2010, 64: 1411 | [24] | XuW S, LiY, WangC X, et al. Analysis on cyclic phase transformation of maraging steel by EBSD [J]. Trans. Mater. Heat Treat., 2014, 35(10): 154 | [24] | 徐文帅, 厉 勇, 王春旭等. 马氏体时效钢循环相变的EBSD分析 [J]. 材料热处理学报, 2014, 35(10): 154 | [25] | QiaoY, ArgonA S. Cleavage crack-growth-resistance of grain boundaries in polycrystalline Fe-2%Si alloy: Experiments and modeling [J]. Mech. Mater., 2003, 35: 129 | [26] | YeliG, AugerM A, WilfordK, et al. Sequential nucleation of phases in a 17-4PH steel: Microstructural characterisation and mechanical properties [J]. Acta Mater., 2017, 125: 38 | [27] | JingC N, FanJ C, WangC L, et al. Characterization and formation mechanism of the weld interface of TRIP590 steel laser welding [J]. Chin. J. Lasers, 2015, 42(4): 57 | [27] | 景财年, 范吉超, 王丛雷等. 激光焊接TRIP590钢焊缝微观结构及形成机理研究 [J]. 中国激光, 2015, 42(4): 57 | [28] | ZhangW Y. Welding Metallurgy [M]. Beijing: Mechanical Industry Stress, 1999: 127 | [28] | 张文钺. 焊接冶金学 [M]. 北京: 机械工业出版社, 1999: 127 | [29] | ZhangM, LiuM Z, ZhangM, et al. Microstructure and mechanical properties of FV520B affected by austenitizing elements Mn and Ni [J]. J. Mater. Eng., 2016, 44(3): 40 | [29] | 张 敏, 刘明志, 张 明等. 奥氏体化合金元素Mn和Ni对FV520B焊缝组织与力学性能的影响 [J]. 材料工程, 2016, 44(3): 40 | [30] | LongS L, LiangY L, JiangY, et al. Effect of quenching temperature on martensite multi-level microstructures and properties of strength and toughness in 20CrNi2Mo steel [J]. Mater. Sci. Eng., 2016, A676: 38 | [31] | Dáz-FuentesM, Iza-MendiaA, GutiérrezI. Analysis of different acicular ferrite microstructures in low-carbon steels by electron backscattered diffraction. Study of their toughness behavior [J]. Metall. Mater. Trans., 2003, 34A: 2505 | [32] | LiaoB, XiaoF R. Research on microstructure and strength-toughening mechanism of acicular ferrite pipeline steel [J]. Trans. Mater. Heat Treat., 2009, 30(2): 57 | [32] | 廖 波, 肖福仁. 针状铁素体管线钢组织及强韧化机理研究 [J]. 材料热处理学报, 2009, 30(2): 57 |
|
|