低压冷喷涂制备Al(Y)-30%Al2O3涂层及其海水腐蚀行为 |
白杨1,2,王振华3,李相波3,李焰1() |
1. 中国石油大学(华东)材料科学与工程学院 青岛 266580 2. 海洋化工研究院有限公司海洋涂料国家重点实验室 青岛 266071 3. 海洋腐蚀与防护重点实验室中船重工七二五所 青岛 266237 |
|
Corrosion Behavior of Al(Y)-30%Al2O3 Coating Fabricated by Low Pressure Cold Spray Technology |
BAI Yang1,2,WANG Zhenhua3,LI Xiangbo3,LI Yan1() |
1. School of Materials Science and Engineering, China University of Petroleum, Qingdao 266580, China 2. State Key Laboratory of Marine Coatings, Marine Chemical Research Institute Co. , Ltd. , Qingdao 266071, China 3. State Key Laboratory for Marine Corrosion and Protection, Luoyang Ship Material Research Institute, Qingdao 266237, China |
引用本文:
白杨, 王振华, 李相波, 李焰. 低压冷喷涂制备Al(Y)-30%Al2O3涂层及其海水腐蚀行为[J]. 金属学报, 2019, 55(10): 1338-1348.
Yang BAI,
Zhenhua WANG,
Xiangbo LI,
Yan LI.
Corrosion Behavior of Al(Y)-30%Al2O3 Coating Fabricated by Low Pressure Cold Spray Technology[J]. Acta Metall Sin, 2019, 55(10): 1338-1348.
[1] | Assadi H, Kreye H, G?rtner F ,et al. Cold spraying-A materials perspective [J]. Acta Mater., 2016, 116: 382 | [2] | Wang C L, Yang S, Ma B, et al. Cold spray technology and its application in parts renewal and preparation of functional coating [J]. Weld. Technol., 2013, 42(8): 1 | [2] | (王存龙, 杨 森, 马 冰等. 冷喷涂技术及其在零件修复与功能涂层制备中的应用 [J]. 焊接技术, 2013, 42(8): 1) | [3] | Irissou E, Legoux J G, Arsenault B ,et al. Investigation of Al-Al2O3 cold spray coating formation and properties [J]. J. Therm. Spray Technol., 2007, 16: 661 | [4] | Rokni M R, Nutt S R, Widener C A ,et al. Review of relationship between particle deformation, coating microstructure, and properties in high-pressure cold spray [J]. J. Therm. Spray Technol., 2017, 26: 1308 | [5] | Melendez N M, Narulkar V V, Fisher G A ,et al. Effect of reinforcing particles on the wear rate of low-pressure cold-sprayed WC-based MMC coatings [J]. Wear, 2013, 306: 185 | [6] | Spencer K, Fabijanic D M, Zhang M X. The influence of Al2O3 reinforcement on the properties of stainless steel cold spray coatings [J]. Surf. Coat. Technol., 2012, 206: 3275 | [7] | Shockley J M, Descartes S, Vo P, et al. The influence of Al2O3 particle morphology on the coating formation and dry sliding wear behavior of cold sprayed Al-Al2O3 composites [J]. Surf. Coat. Technol., 2015, 270: 324 | [8] | Shockley J M, Descartes S, Irissou E ,et al. Third body behavior during dry sliding of cold-sprayed Al-Al2O3 composites: In situ tribometry and microanalysis [J]. Tribol. Lett., 2014, 54: 191 | [9] | Winarto W, Priadi D, Sofyan N ,et al. Wear resistance and surface hardness of carbon nanotube reinforced alumina matrix nanocomposite by cold sprayed process [J]. Procedia Eng., 2017, 170: 108 | [10] | Tao Y S, Xiong T Y, Sun C ,et al. Effect of α-Al2O3 on the properties of cold sprayed Al/α-Al2O3 composite coatings on AZ91D magnesium alloy [J]. Appl. Sur. Sci., 2009, 256: 261 | [11] | Peat T, Galloway A, Toumpis A, et al. The erosion performance of particle reinforced metal matrix composite coatings produced by co-deposition cold gas dynamic spraying [J]. Appl. Sur. Sci., 2017, 396: 1623 | [12] | Bai X M, Tang J Q, Gong J M ,et al. Corrosion performance of Al-Al2O3 cold sprayed coatings on mild carbon steel pipe under thermal insulation [J]. Chin. J. Chem. Eng., 2017, 25: 533 | [13] | Liang X B, Zhang Z B, Chen Y X, et al. Study on Al-based amorphous and nanocrystalline composite coating [J]. Acta Metall. Sin., 2012, 48: 289 | [13] | (梁秀兵, 张志彬, 陈永雄等. 铝基非晶纳米晶复合涂层研究 [J]. 金属学报, 2012, 48: 289) | [14] | Luo L, Shen Y F, Li B ,et al. Preparation and oxidation behavior of alu-minized coating on TC4 titanium alloy via friction stir lap welding method [J]. Acta Metall. Sin., 2013, 49: 996 | [14] | (骆 蕾, 沈以赴, 李 博等. 搅拌摩擦焊搭接法制备TC4钛合金表面Al涂层及其高温氧化行为 [J]. 金属学报, 2013, 49: 996) | [15] | Su F, Zhang P Z, Wei D B ,et al. Corrosion behavior of hot-dip Al-Zn coating doped with Si, RE, and Mg during exposure to sodium chloride containing environments [J]. Mater. Corros., 2018, 69: 714 | [16] | Ma J L, Wen J B, Li G X ,et al. The corrosion behaviour of Al-Zn-In-Mg-Ti alloy in NaCl solution [J]. Corros. Sci., 2010, 52: 534 | [17] | Liu Z, Xu H Q, Zhi W ,et al. Mechanical properties and corrosion behavior of Al/SiC composites [J]. J. Alloys Compd., 2016, 678: 23 | [18] | Che X, Liang X K, Chen L L ,et al. Microstructures and low-cycle fatigue behavior of Al-9.0%Si-4.0%Cu-0.4%Mg(-0.3%Sc) alloy[J]. Acta Metall. Sin., 2014, 50: 1046 | [18] | (车 欣, 梁兴奎, 陈丽丽等. Al-9.0%Si-4.0%Cu-0.4%Mg (-0.3%Sc)合金的显微组织及其低周疲劳行为 [J]. 金属学报, 2014, 50: 1046) | [19] | Liu W, Li Q, Li M C. Corrosion behaviour of hot-dip Al-Zn-Si and Al-Zn-Si-3Mg coatings in NaCl solution [J]. Corros. Sci., 2017, 121: 72 | [20] | Wang K. Corrosion behavior of cold-sprayed aluminum and zinc/aluminum coatings serviced in marine atmosphere environment [D]. Jinan: Shandong University, 2011 | [20] | (王 凯. 冷喷涂铝及铝锌涂层海洋大气腐蚀行为研究 [D]. 济南: 山东大学, 2011) | [21] | Jiang Q, Miao Q, Liang W P, et al. Corrosion behavior of arc sprayed Al-Zn-Si-RE coatings on mild steel in 3.5 wt% NaCl solution [J]. Electrochim. Acta, 2014, 115: 644 | [22] | Tao Y S, Xiong T Y, Sun C ,et al. Microstructure and corrosion performance of a cold sprayed aluminium coating on AZ91D magnesium alloy [J]. Corros. Sci., 2010, 52: 3191 | [23] | Dong C F, Fu A Q, Li X G ,et al. Localized EIS characterization of corrosion of steel at coating defect under cathodic protection [J]. Electrochim. Acta, 2008, 54: 628 | [24] | Fu D X. Study on the synergy effect between Zn-Al-Mg-RE coating and ship paint and anticorrosion mechanism of the composite coatings [D]. Harbin: Harbin Engineering University, 2007 | [24] | (付东兴. Zn-Al-Mg-RE涂层与舰船涂料的协同性及其构建的复合涂层的耐蚀机理研究 [D]. 哈尔滨: 哈尔滨工程大学, 2007) | [25] | Li T, Li X G, Dong C F ,et al. Initial corrosion behavior of LC4 aluminum alloy in tropical maritime environment [J]. J. Univ Sichuan. (Nat Sci. Ed.), 2010, 47: 1388 | [25] | (李 涛, 李晓刚, 董超芳等. LC4铝合金在热带海洋大气环境中的早期腐蚀行为 [J]. 四川大学学报(自然科学版), 2010, 47: 1388) | [26] | Wang Z Y, Li Q X, Wang C, et al. Corrosion behaviors of Al alloy LC4 in Geermu salt lake atmosphere [J]. Chin. J. Nonferrous Met., 2007, 17: 24 | [26] | (王振尧, 李巧霞, 汪 川 ,等. LC4铝合金在格尔木盐湖大气环境中的腐蚀行为 [J]. 中国有色金属学报, 2007, 17: 24) | [27] | Nyquist R A, Kagel R O. Infrared Spectra of Inorganic Compounds (3800-45cm-1) [M]. New York: Academic Press, 1971: 1 | [28] | He J G, Wen J B, Sun L M ,et al. Characterization of pitting behavior of pure Al and Al-7Zn-0.1Sn-0.015Ga alloy by cyclic polarization technique [J]. Corros. Sci. Prot. Technol., 2015, 27: 449 | [28] | (贺俊光, 文九巴, 孙乐民等. 用循环极化曲线研究Al和铝合金的点蚀行为 [J]. 腐蚀科学与防护技术, 2015, 27: 449) | [29] | Davoodi A, Pan J, Leygraf C ,et al. Integrated AFM and SECM for in situ studies of localized corrosion of Al alloys [J]. Electrochim. Acta, 2007, 52: 7697 | [30] | Wu L W. Investigation on microstructure and properties of Al, Ti-Al-N, Al/Ti-Al-N films fabricated on AZ91D magnesium alloy by magnetron sputtering [D]. Zhenjiang: Jiangsu University of Science and Technology, 2011 | [30] | (吴良文. AZ91D镁合金表面磁控溅射Al、Ti-Al-N、Al/Ti-Al-N膜及其组织与性能研究 [D]. 镇江: 江苏科技大学, 2011) | [31] | Zhu Z X, Zhang J, Xu B S. Effect of RE on anti-corrosion mechanism of arc sprayed Zn-Al-Mg coatings [J]. Adv. Mater. Res., 2011, 282-283: 279 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|