高碳钢连铸方坯拉坯方向偏析C元素分布的时间序列波动特征 |
侯自兵(), 徐瑞, 常毅, 曹江海, 文光华, 唐萍 |
重庆大学材料科学与工程学院 重庆 400044 |
|
Time-Series Fluctuation Characteristics of Segregation Carbon Element Distribution Along Casting Direction in High Carbon Continuous Casting Billet |
Zibing HOU(), Rui XU, Yi CHANG, Jianghai CAO, Guanghua WEN, Ping TANG |
College of Materials Science and Engineering, Chongqing University, Chongqing 400044, China |
引用本文:
侯自兵, 徐瑞, 常毅, 曹江海, 文光华, 唐萍. 高碳钢连铸方坯拉坯方向偏析C元素分布的时间序列波动特征[J]. 金属学报, 2018, 54(6): 851-858.
Zibing HOU,
Rui XU,
Yi CHANG,
Jianghai CAO,
Guanghua WEN,
Ping TANG.
Time-Series Fluctuation Characteristics of Segregation Carbon Element Distribution Along Casting Direction in High Carbon Continuous Casting Billet[J]. Acta Metall Sin, 2018, 54(6): 851-858.
[1] | Weng Y Q.China's economic development on the demand for some high-end steel products [A]. The Chinese Society for Metals. Ninth China Iron and Steel Annual Conference [C]. Beijing: Metallurgical Industry Press, 2013: 12(翁宇庆. 我国经济发展对部分高端钢铁品种的需求 [A]. 中国金属学会. 第九届中国钢铁年会论文集[C]. 北京:冶金工业出版社, 2013: 12) | [2] | Choudhary S K, Ganguly S.Morphology and segregation in continuously cast high carbon steel billets[J]. ISIJ Int., 2007, 47: 1759 | [3] | Li Y X, Liao M, Li B C, et al.High-carbon steel production process and quality analysis[J]. Steelmaking, 2009, 25(4): 1(李永祥, 廖明, 李碧春等. 高碳钢生产工艺及质量分析[J]. 炼钢, 2009, 25(4): 1) | [4] | Flemings M C.Our understanding of macrosegregation: Past and present[J]. ISIJ Int., 2000, 40: 833 | [5] | Lesoult G. Macrosegregation in steel strands and ingots:Characterisation,formation and consequences [J]. Mater. Sci. Eng., 2005, A413-414: 19 | [6] | Cai Z Z, Zhu M Y.Microsegregation of solute elements in solidifying mushy zone of steel and its effect on longitudinal surface cracks of continuous casting strand[J]. Acta Metall. Sin., 2009, 45: 949(蔡兆镇, 朱苗勇. 钢凝固两相区溶质元素的微观偏析及其对连铸坯表面纵裂纹的影响[J]. 金属学报, 2009, 45: 949) | [7] | Han Z Q, Cai K K.Study on a mathematical model of microsegregation in continuously cast slab[J]. Acta Metall. Sin., 2000, 36: 869(韩志强, 蔡开科. 连铸坯中微观偏析的模型研究[J]. 金属学报, 2000, 36: 869) | [8] | Ludlow V, Normanton A, Anderson A, et al.Strategy to minimise central segregation in high carbon steel grades during billet casting[J]. Ironmaking Steelmaking, 2005, 32: 68 | [9] | Tacke K H.Cavity sequences in continuously cast billets: Part II. Stochastic models[J]. Metall. Mater. Trans., 1999, 30B: 763 | [10] | Choudhary S K, Ganguly S.Morphology and segregation in continuously cast high carbon steel billets[J]. ISIJ Int., 2007, 47: 1759 | [11] | Chang Y, Hou Z B, Wang W, et al.Characteristics and mechanism of carbon element and manganese element distribution along casting direction in high-carbon billet[J]. Iron Steel, 2016, 51(11): 43(常毅, 侯自兵, 王伟等. 高碳钢方坯碳锰元素纵向分布及机理[J]. 钢铁, 2016, 51(11): 43) | [12] | Yuan X F, Sun S Q.Introduce the standard figure of GB/T 1979-2001 structure steel macrostructure and defect[J]. Metall. Standard. Qual., 2002, 40(6): 8(袁辛芳, 孙时秋. GB/T 1979-2001 结构钢低倍组织缺陷评级图介绍[J]. 冶金标准化与质量, 2002, 40(6): 8) | [13] | Cai K K.Quality Control of Continuously Cast Steel [M]. Beijing: Metallurgical Industry Press, 2010: 283(蔡开科. 连铸坯质量控制 [M]. 北京: 冶金工业出版, 2010: 283) | [14] | Chen Y, Yang S B, Zhu M Y.Key technologies of internal quality control for continuously cast high-speed rail steel bloom[J]. Iron Steel, 2006, 41(12): 36(陈永, 杨素波, 朱苗勇. 高速轨用钢连铸坯内部质量控制的关键技术[J]. 钢铁, 2006, 41(12): 36) | [15] | Li P, Wang L, Zhou Q F.Formation reasons and countermeasures of cementite network in the Center of 82B wire rods[J]. J. Iron Steel Res., 2014, 26(9): 33(李平, 王雷, 周青峰. 82B中心网状渗碳体产生原因及改善方法[J]. 钢铁研究学报, 2014, 26(9): 33) | [16] | Box G E P, Jenkins G M, Reinsel G C. Time Series Analysis: Forecasting and Control[M]. 4th Ed., Hoboken: Wiley, 2008: 2 | [17] | Hou Z B, Cheng G G, Wu C C, et al.Time-series analysis technologies applied to the study of carbon element distribution along casting direction in continuous-casting billet[J]. Metall. Mater. Trans., 2012, 43B: 1517 | [18] | Hou Z B, Wen G H, Tang P, et al.Periodicity of carbon element distribution along casting direction in continuous-casting billet by using singular spectrum analysis[J]. Metall. Mater. Trans., 2014, 45B: 1817 | [19] | Wang H Z.Original position statistic distribution analysis (original position analysis): A new analytical method in research and quality evaluation of materials[J]. Sci. China, 2003, 46B: 119 | [20] | Yang S Z, Wu Y, Xuan J P, et al.Time Series Analysis in Engineering Application (Volume II) [M]. 2nd Ed., Wuhan: Huazhong University of Science and Technology Press, 2007: 1(杨叔子, 吴雅, 轩建平等. 时间序列分析的工程应用(下册) [M]. 第2版. 武汉: 华中科技大学出版社, 2007: 1) | [21] | Trivedi R, Kurz W.Dendritic growth[J]. Int. Mater. Rev., 1994, 39: 49 | [22] | Ganguly S, Choudhary S K.Quantification of the solidification microstructure in continuously-cast high-carbon steel billets[J]. Metall. Mater. Trans., 2009, 40B: 397 | [23] | Feng J, Chen W Q.Influential factors of primary dendritic arm spacing in high-carbon steel billets[J]. J. Univ. Sci. Technol. Beijing, 2007, 29(1): 25(冯军, 陈伟庆. 高碳钢小方坯的一次枝晶臂间距的影响因素[J]. 北京科技大学学报, 2007, 29(1): 25) | [24] | Hu Z Y, Chen X H, Tang P,et al.Effect of superheat on carbon segregation in continuous casting billet of cord steel[J]. Continu. Cast., 2017, (5): 12(胡志勇, 陈兴华,唐萍等. 过热度对帘线钢连铸方坯碳偏析的影响[J]. 连铸, 2017, (5): 12) | [25] | Tomono H, Hitomi Y, Ura S.Mechanism of formation of the V-shaped segregation in the large section continuous cast bloom[J]. Trans. Iron Steel Inst Japan, 1984, 24: 917 | [26] | Lai C B, Xin B, Chen W Q, et al.Effect of secondary dendritic arm spacing on center carbon segregation of slab[J]. Steelmaking, 2009, 25(4): 42(赖朝彬, 辛博, 陈伟庆等. 连铸板坯二次枝晶臂间距对中心碳偏析的影响[J]. 炼钢, 2009, 25(4): 42) | [27] | Tian L, Jiang H.The Effect of solidification structures on central segregation of slabs[J]. Continu. Cast., 2010, (1): 26(田陆, 江浩. 凝固组织对连铸板坯中心偏析的影响[J]. 连铸, 2010, (1): 26) | [28] | Xu X J, Deng A Y, Wang E G, et al.Effect mechanism of high frequency electromagnetic field on the surface quality and equiaxed crystal ratio of 15CrMo Billet[J]. Acta Metall. Sin., 2009, 45: 1330(许秀杰, 邓安元, 王恩刚, 等. 高频电磁场对15CrMo连铸坯表面质量和等轴晶率的影响机理[J]. 金属学报, 2009, 45: 1330) |
|
|