GexSe90-xSb10硫系玻璃的热力学特性和动力学脆性研究* |
李姣姣,坚增运(),朱满,许军锋,常芳娥,相敏 |
|
STUDY ON THERMODYNAMIC PROPERTIES AND KINETICS FRAGILITY OF GexSe90-xSb10 CHALCOGENIDE GLASSES |
Jiaojiao LI,Zengyun JIAN,Man ZHU,Junfeng XU,Fang'e CHANG,Min XIANG |
School of Materials and Chemical Engineering, Xi'an Technological University, Xi'an 710021 |
引用本文:
李姣姣,坚增运,朱满,许军锋,常芳娥,相敏. GexSe90-xSb10硫系玻璃的热力学特性和动力学脆性研究*[J]. 金属学报, 2015, 51(11): 1384-1390.
Jiaojiao LI,
Zengyun JIAN,
Man ZHU,
Junfeng XU,
Fang'e CHANG,
Min XIANG.
STUDY ON THERMODYNAMIC PROPERTIES AND KINETICS FRAGILITY OF GexSe90-xSb10 CHALCOGENIDE GLASSES[J]. Acta Metall Sin, 2015, 51(11): 1384-1390.
[1] | Angell C A. Science, 1995; 267: 1924 | [2] | Fontana G D, Battezzati L. Acta Mater, 2013; 61: 2260 | [3] | Mukherjee S, Schroers J, Johnson W L, Rhim W K. Phys Rev Lett, 2005; 94: 245501 | [4] | Turnbull D. Contemp Phys, 1969; 10: 473 | [5] | Kauzmann W. Chem Rev, 1948; 43: 219 | [6] | Jian Z Y, Zhou J, Chang F E, Jie W Q. Acta Metall Sin, 1999; 45: 1146 (坚增运, 周 晶, 常芳娥, 介万奇. 金属学报, 1999; 45: 1146) | [7] | Debenedetti P G, Stillinger F H. Nature, 2001; 410: 259 | [8] | Gibson J M. Science, 2009; 326: 942 | [9] | Angell C A. J Non-Cryst Solids, 1985; 73: 1 | [10] | Cai A H, Ding D W, Xiong X, Liu Y, An W K, Zhou G J, Luo Y, Li T L, Li X S. Mater Des, 2014; 63: 233 | [11] | Gallino I, Schroers J, Busch R. J Appl Phys, 2010; 108: 063501 | [12] | Jiang Q K, Wang X D, Nie X P, Zhang G Q, Ma H, Fecht H J,Bendnarcik J, Franz H, Liu Y G, Cao Q P, Jiang J Z. Acta Mater, 2008; 56: 1785 | [13] | Battezzati L, Castellero A, Rizzi P. J Non-Cryst Solids, 2007; 353: 3318 | [14] | Battezzati L. Rev Adv Mater Sci, 2008; 18: 184 | [15] | Glade S C, Busch R, Lee D S, Johnson W L, Wunderlich R K, Fecht H J. J Appl Phys, 2000; 87: 7242 | [16] | Evenson Z, Busch R. Acta Mater, 2011; 59: 4404 | [17] | Jiang Q, Xu X Y, Li J C. Acta Metall Sin, 1997; 33: 6 (蒋 青, 徐晓亚, 李建忱. 金属学报, 1997; 33: 6) | [18] | Legg B A, Schroers J, Busch R. Acta Mater, 2007; 55: 1109 | [19] | Jia R, Bian X F, Wang Y Y. Chin Sci Bull, 2011; 56: 3912 | [20] | Lu Z P, Li Y, Liu C T. J Appl Phys, 2003; 93: 286 | [21] | Senkov O N. Phys Rev, 2007; 76B: 104202 | [22] | Jiang Q K, Zhang G Q, Yang L, Wang X D, Saksl K, Franz H,Wunderich R, Fecht H, Jiang J Z. Acta Mater, 2007; 55: 4409 | [23] | Fiore G, Battezzati L. J Alloys Compd, 2009; 483: 54 | [24] | Fan G J, L?ffler J F, Wunderlich R K, Fecht H J. Acta Mater, 2004; 52: 667 | [25] | Zhu M, Li J J, Yao L J, Jian Z Y, Chang F E, Yang G C. Thermochim Acta, 2013; 565: 132 | [26] | Gallino I, Gross O, Fontana G D, Evenson Z, Busch R. J Alloys Compd , 2014; 615: S35 | [27] | Zhang X H, Guimond Y, Bellec Y. J Non-Cryst Solids, 2003; 326: 519 | [28] | Varshneya A K, Mauro D J. J Non-Cryst Solids, 2007; 353: 1291 | [29] | Vázquez J, Barreda D G, López-Alemany P L, Villares P, Jiménez-Garay R. J Alloys Compd, 2005; 390: 94 | [30] | Lee J H, Lee W H, Park J K, Yi J H, Shin S Y, Park B J, So B, Heo J, Choi J H, Kim H J, Choi Y G. J Non-Cryst Solids, doi: | [31] | Soltana A S, Abu-Sehly A A, Joraid A A, Alamri S N. Thermochim Acta, 2013; 574: 73 | [32] | Tlchy L, Tichá H. J Non-Cryst Solids, 1995; 189: 141 | [33] | Guo H, Tao H Z, Gong Y Q, Zhao X J. J Non-Cryst Solids, 2008; 354: 1159 | [34] | Dinsdale A T. Calphad, 1991; 15: 317 | [35] | Angell C A. MRS Bull, 2008; 33: 544 | [36] | Martinez L M, Angell C A. Nature, 2001; 410: 663 | [37] | Ito K, Moynihan C T, Angell C A. Nature, 1999; 398: 492 | [38] | Angell C A. J Non-Cryst Solids, 1988; 102: 205 | [39] | Kissinger H E. Anal Chem, 1957; 29: 1702 | [40] | Rabinal M K, Sangunni K S, Gopal E S R. J Non-Cryst Solids, 1995; 188: 98 | [41] | Zhang C Z. PhD Dissertation, Shandong University, Jinan, 2011 (张春芝. 山东大学博士学位论文, 济南, 2011) | [42] | Guo Y F, Yavari A R, Zhang T. J Alloys Compd, 2012; 536: 91 | [43] | Angell C A. Physica, 1997; 107D: 122 | [44] | Sreeram A N, Varshneya A K, Swiler D R. J Non-Cryst Solids, 1991; 128: 294 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|